Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 400 µm | 400 µm | SABIC Method |
SABIC Innovative Plastics Cycolac® INP449 ABS+SAN SABIC INP449 is a T-SAN (Teflon (PTFE)-Styrene-Ancrylonitrile) resin for use as an FR anti-drip agent |
|||
Particle Size | 400 µm | 400 µm | mean resin; SABIC Method |
SABIC Innovative Plastics Cycolac® INP449 SAN SABIC INP449 is a T-SAN (Teflon (PTFE)-Styrene-Ancrylonitrile) resin for use as an FR anti-drip agentThis data was supplied by SABIC-IP for the Americas region. |
|||
Particle Size | 400 - 750 µm | 400 - 750 µm | |
Polimeri Europa Extir® EH 2000 Expandable Polystyrene Extir EH 2000 is an expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 2000 is use.. |
|||
Particle Size | 400 - 750 µm | 400 - 750 µm | |
Polimeri Europa Extir® LN 2001 Expandable Polystyrene Extir LN 2001 belongs to a new expandable product family, the Leonardo Series. Extir LN 2001 is specially coated to be incorporated into bricks, concrete, mortar and plaster, in order to lighten the.. |
|||
Particle Size | 400 - 750 µm | 400 - 750 µm | |
Polimeri Europa Extir Leonardo B 2000 AE Expandable Polystyrene
(discontinued **) Extir B 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir B 200.. |
|||
Particle Size | 400 - 750 µm | 400 - 750 µm | |
Polimeri Europa Extir® E 2000 AE Expandable Polystyrene
(discontinued **) Extir E 2000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Thi.. |
|||
Particle Size | 400 - 570 µm | 400 - 570 µm | Average value: 501 µm Grade Count:15 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |
|||
Particle Size | <= 400 µm | <= 400 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5018 400 Micron LDPE Powder Description: ICOFLO 510-5018 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 400 µm | <= 400 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5020 400 Micron LDPE Powder Description: ICOFLO 510-5020 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 400 µm | <= 400 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5023 400 Micron LDPE Powder Description: ICOFLO 510-5023 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 400 µm | <= 400 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5028 400 Micron LLDPE Powder Description: ICOFLO 510-5028 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 400 µm | <= 400 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5049 400 Micron LDPE Powder Description: ICOFLO 510-5049 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 400 µm | <= 400 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5069 400 Micron LLDPE Powder Description: ICOFLO 510-5069 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | 400 - 630 µm | 400 - 630 µm | |
SYNTHOS Koplen® 0207 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into thin walled products.Specific Characteristics: Flammability according .. |
|||
Particle Size | 400 - 630 µm | 400 - 630 µm | |
SYNTHOS Koplen® 0207 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to thin-wall moldings. Lower density can be achie.. |
|||
Particle Size | 400 µm | 400 µm | Average Mean |
SPHERE ONE EXTENDOSPHERESâ„¢ 300/600 Hollow Spheres EXTENDOSPHERESâ„¢300/600 are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, they can .. |
|||
Particle Size | 400 µm | 400 µm | Average |
Daikin POLYFLON FA-500 MPA, White Powder White powder.Major Uses: Addition of a minute amount of resins produces excellent anti-dripping properties. Good dispersion into resins enables production of moldings with better appearance than wi.. |
|||
Particle Size | 400 µm | 400 µm | Laser Method (Dry) |
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces.. |
|||
Particle Size | 400 µm | 400 µm | ASTM D4894 |
Daikin POLYFLON M-392 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding, automatic or semi-automatic compression molding, isostatic molding, and ram extrusion.Features: Good fill characteristics particularly into .. |
|||
Particle Size | 400 - 800 µm | 400 - 800 µm | grain size; 400lambda - 800lambda |
China-Yixing Longly Refractories Zirconia Ceramics LONGLY provides a multitude of zirconia products including balls, plates, tubes, rods and etc. by adopting magnesia, calcia or yttria stabilized zirconia powder as raw material through dry pressing,.. |
|||
Particle Size | >= 400 µm | >= 400 µm | 0.28 |
Arkema Group OREVAC® 18350P Grafted Maleic Anhydride Polyethylene OREVAC 18350P is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE and HDPE coating for steel pipeline. It is mainly used in pipe coating to have good adhesion pe.. |
|||
Particle Size | >= 400 µm | >= 400 µm | 0.05 |
Arkema Group OREVAC® 18510P Grafted Maleic Anhydride Polyethylene OREVAC 18510P is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510P is mainly used in pip.. |
|||
Particle Size | >= 400 µm | >= 400 µm | 0 |
Arkema Group OREVAC® 18732 Grafted Maleic Anhydride Polypropylene OREVAC 18732 and 18732P are maleic anhydride grafted polypropylene used in the manufacturing of multiplayer structures. These products are available in pellets or in powder. OREVAC 18732 and 18732P .. |
|||
Particle Size | >= 400 µm | >= 400 µm | 0 |
Arkema Group OREVAC® 18732P Grafted Maleic Anhydride Polypropylene OREVAC 18732 and 18732P are maleic anhydride grafted polypropylene used in the manufacturing of multiplayer structures. These products are available in pellets or in powder. OREVAC 18732 and 18732P .. |
|||
Particle Size | 400 - 1200 µm | 400 - 1200 µm | Average value: 771 µm Grade Count:7 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m.. |
|||
Particle Size | 400 - 750 µm | 400 - 750 µm | |
Polimeri Europa Extir® LN 2000 Expandable Polystyrene Extir LN 2000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion.. |
|||
Particle Size | 400 - 750 µm | 400 - 750 µm | |
Polimeri Europa Extir Leonardo A 2000 AE Expandable Polystyrene
(discontinued **) Extir A 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 200.. |