Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 3.0 µm | >= 3.0 µm | 10% smaller than |
Nyco ASPECT® 3000 Wollastonite High aspect ratio grade. It is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. .. |
|||
Particle Size | >= 3.0 µm | >= 3.0 µm | 10% smaller than |
Nyco NYAD® MD325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Particle Size | >= 3.0 µm | >= 3.0 µm | 10% smaller than |
Nyco NYGLOS® M3 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | >= 3.0 µm | >= 3.0 µm | Primary Crystal Size |
Nabaltec NABALOX® NO 115-71 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 3.0 µm | 3.0 µm | Median Grain Diameter |
Nabaltec NABALOX® NO 325 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | First Grade |
Oceanchem Group Zinc Borate Information Provided by Oceanchem Group |
|||
Particle Size | 3.0 - 4.0 µm | 3.0 - 4.0 µm | Primary |
NYC YT3X Y2O3 Powder |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 3.0 µm | 3.0 µm | d90 |
Magyar Aluminum ALO-DN-7P Alumina Ground Alumina |
|||
Particle Size | 3.0 µm | 3.0 µm | d90 |
Magyar Aluminum ALO-EL-7P Alumina Ground Alumina |
|||
Particle Size | 3.0 - 6.0 µm | 3.0 - 6.0 µm | d50 |
Magyar Aluminum ALOLT 50AF Aluminum Hydroxide Ground type |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | average |
Malvern Minerals Novacite® L-207A Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | average |
Malvern Minerals Novakup® L-207A Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | |
Manufacturing Insight EFR-1FM Enhanced Fire Retardant Additive EFR-1FM is ideal for incorporation into reinforced (carbon fiber, Kevlar fiber, glass fiber) thermoset resin systems, including coatings and foams, potting compounds, fiberglass reinforced structure.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% |
Minelco UltraCarb LH15X Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | <= 3.0 µm | <= 3.0 µm | Fineness of Grind |
Gwent Electronic Materials C2050425D1 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |
|||
Particle Size | 3.0 µm | 3.0 µm | Crystal Size |
Momentive Performance Materials HCPH Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powders of grades HCP, HCPH, HCPL, and AC6004 are generally single-crystal hexagonal platelets with very high purity. The mean particle sizes for these ultra-.. |
|||
Particle Size | 3.0 - 6.0 µm | 3.0 - 6.0 µm | mean; 100% -325 mesh |
Momentive Performance Materials HCT-F Titanium Diboride (TiB2) Powder Grade HCT-F powders are designed for use on applications requiring reduced particle size without sacrificing high purity.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced.. |
|||
Particle Size | 3.0 - 6.0 µm | 3.0 - 6.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade D Titanium Diboride, TiB2 Powder for hot pressing, technical grade.Hot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous met.. |
|||
Particle Size | 3.0 - 6.0 µm | 3.0 - 6.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade SE Titanium Diboride, TiB2 Higher N, O, Fe contentsHot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous metalsCeramic shapes.. |
|||
Particle Size | <= 3.0 µm | <= 3.0 µm | |
Ferro EG 2992 Glaze and Sealant Glass Glass Type: Bi-Zn-B Typical Powder Form: SRRG Typical Application: Ferrites Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insu.. |
|||
Particle Size | 3.0 µm | 3.0 µm | D10 (Malvern) Size C |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 3.0 µm | 3.0 µm | |
Dow Corning 9506 Powder A spherical white powder comprised of dimethicone / vinyl dimethicone crosspolymer for use in skincare, suncare, and color cosmetic applications.Information provided by Dow Corning |
|||
Particle Size | 3.0 - 4.0 µm | 3.0 - 4.0 µm | |
Dow Corning PF-2520 ELASTOMER EMULSION DOW CORNING® PF-2520 Elastomer Emulsion has been developed to facilitate the incorporation of an elastomeric powder in fluid into water-based silicone powder into water-based cosmetic products. It .. |
|||
Particle Size | 3.0 - 10 µm | 3.0 - 10 µm | Thin Section Crystal Size |
CoorsTek Pure SiC™ LR CVD Silicon Carbide, > 99.9995% Data Provided by the manufacturer, CoorsTek, Inc. |
|||
Particle Size | 3.0 µm | 3.0 µm | D50 |
Dandong Taico Minerals TAICOCITE® TC35 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Particle Size | 3.0 µm | 3.0 µm | Median |
CIMBAR CIMBAR™ XF Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | Medium Grain (d50) |
CeramTec CeramCool® Rubalit® 708 Alumina, 96% CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles |
Ferro EG 2964 Glaze and Sealant Glass Glass Type: Bi-Zn-B Typical Powder Form: VWG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ins.. |
|||
Particle Size | 3.0 µm | 3.0 µm | Maximum of 3% less than |
H.C. Starck Amperit® 335.066 Nickel Self-fluxing Alloy HRC 60 (NiCrBSi) |