Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 2000 µm | <= 2000 µm | Max size of 99% of particles; Sieve Analysis |
Polimeri Europa Europrene® N 3380/P Acrylonitrile-Butadiene Rubber Europrene® N 3380/P is a powdered acrylonitrile-butadiene copolymer which is cold polymerized. During the production process, a non staining antioxidant is added while a mineral antistick agent is.. |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | Average value: 3000 µm Grade Count:4 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Particle Size | <= 2000 µm | <= 2000 µm | Grain Size |
Gouda Vuurvast CURON 180 TF Dense Refractory Castable Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark.. |
|||
Particle Size | 2000 - 3000 µm | 2000 - 3000 µm | Diameter per caliper rule |
Stanelco Bioplast® GS 2189 Biodegradable Plastic Bioplast 2189 is a product that is optimised for sheet extrusion, injection and compression moulding. It is always biodegradable and readily compostable in thin sections, this material is useable i.. |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | chip length |
Voloknohim Nylon 6 Chips A Grade Packing: Nylon 6 is packed in 650 kg big-bags on palletsInformation provided by Voloknokhim |
|||
Particle Size | 2000 - 5000 µm | 2000 - 5000 µm | at least 97% |
Voloknohim PA-SV30 Glass and Mineral Filled Information provided by Voloknokhim |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | Pellet Size |
Axion Polymers Axpoly® PP06 5001 Enhanced Black General Purpose Polypropylene PP06 Series polypropylene offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PP06 range of resin co.. |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | Pellet Size |
Axion Polymers Axpoly® PS01 3003 Enhanced White General Purpose Polystyrene PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co.. |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | Pellet Size |
Axion Polymers Axpoly® PS01 3009 Green General Purpose Polystyrene PS01 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of resin co.. |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | Pellet Size |
Axion Polymers Axpoly® PS01 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from refrigerators)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in a range of co.. |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | Pellet Size |
Axion Polymers Axpoly® PS02 1000 General Purpose Polystyrene PS02 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin com.. |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | Pellet Size |
Axion Polymers Axpoly® PS02 1010 Medium Impact Polystyrene PS02 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin co.. |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | Pellet Size |
Axion Polymers Axpoly® PS02 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from television casings)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/gr.. |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | Pellet Size |
Axion Polymers Axpoly® PS13 1000 Impact Modified Polystyrene PS13 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS13 range of resin co.. |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | Pellet Size |
Axion Polymers Axpoly® PS13 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from coat hangers)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/greyCost.. |
|||
Particle Size | >= 2000 µm | >= 2000 µm | |
BASF Neopolen® P 8220 K 0.02 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to.. |
|||
Particle Size | >= 2000 µm | >= 2000 µm | |
BASF Neopolen® P 8220 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to.. |
|||
Particle Size | >= 2000 µm | >= 2000 µm | |
BASF Neopolen® P 8225 K 0.025 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Particle Size | >= 2000 µm | >= 2000 µm | |
BASF Neopolen® P 8225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Particle Size | >= 2000 µm | >= 2000 µm | |
BASF Neopolen® P 8225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Particle Size | >= 2000 µm | >= 2000 µm | |
BASF Neopolen® P 8225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | Pellet Size |
Axion Polymers Axpoly® PS01 3000 General Purpose Polystyrene PS01 Series polystyrenes offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS01 range of custom co.. |
|||
Particle Size | 2000 - 4000 µm | 2000 - 4000 µm | Pellet Size |
Axion Polymers Axpoly® PS13 1011 High Impact Polystyrene PS13 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS13 range of resin co.. |
|||
Particle Size | 2000 - 5000 µm | 2000 - 5000 µm | at least 97% |
Voloknohim PA-TM15 Glass and Mineral Filled Information provided by Voloknokhim |
|||
Particle Size | >= 2000 µm | >= 2000 µm | |
BASF Neopolen® P 8220 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to.. |