Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1400 - 2200 µm | 1400 - 2200 µm | |
Polimeri Europa Extir® LN 7000 Expandable Polystyrene Extir LN 7000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strenght, e.. |
|||
Particle Size | 1400 - 2200 µm | 1400 - 2200 µm | |
Polimeri Europa Extir Leonardo A 7000 AE Expandable Polystyrene
(discontinued **) Extir A 7000 AE is a flame retardant expandable polystyrene in the form of spherical beads of large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 7.. |
|||
Particle Size | >= 1400 µm | >= 1400 µm | <3% |
Solvay Chemicals Oxyper® S131 Sodium Percarbonate Oxyper® S131 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products and environmental applications; it may be suitabl.. |
|||
Particle Size | >= 1400 µm | >= 1400 µm | <10% |
Solvay Chemicals Oxyper® S142 Sodium Percarbonate Oxyper® S142 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in formulated bleach additive products, detergent powders and tablets, automa.. |
|||
Particle Size | >= 1400 µm | >= 1400 µm | <10% |
Solvay Chemicals Oxyper® SHC Sodium Percarbonate Oxyper® SHC is a high coated, stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products, detergent powders and tablets, autom.. |
|||
Particle Size | <= 1400 µm | <= 1400 µm | on #35 Mesh; RP-0499 |
Solvay REPEL-O-TEX® SF2 Surfactant Description: High active soil release polymer for powder laundry. Prevents adhesion of soils between washes and soil redeposition during wash. Repel-O-Tex SF2 has been specifically formulated for im.. |
|||
Particle Size | 1400 - 2000 µm | 1400 - 2000 µm | |
Potters Industries A-Series A-170 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |