Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.30 - 0.50 µm | 0.30 - 0.50 µm | Primary |
NYC YT3W Y2O3 Powder |
|||
Particle Size | 0.30 - 0.50 µm | 0.30 - 0.50 µm | Primary |
NYC YT3WP Y2O3 Granules |
|||
Particle Size | 0.30 µm | 0.30 µm | median |
Imerys Aftonâ„¢ Kaolin Afton is a fine-grained air floating kaolin which is widely used as an anit-caking agent in certain agricultural compounds.Information provided by Imerys |
|||
Particle Size | 0.30 µm | 0.30 µm | median |
Imerys Aftonâ„¢ R Kaolin Afton is a fine-grained kaolin used asa a filler in hard rubber products, plastic products, adhesives, protective coatings and similar applications.Information provided by Imerys |
|||
Particle Size | 0.30 µm | 0.30 µm | median |
Imerys Amlockâ„¢ 321 Kaolin Information provided by Imerys |
|||
Particle Size | 0.30 µm | 0.30 µm | median |
Imerys Bardenâ„¢ Kaolin Barden is a high surface area kaolin product used a filler in rubber and plastic applications.Information provided by Imerys |
|||
Particle Size | 0.30 µm | 0.30 µm | median |
Imerys Bardenâ„¢ R Kaolin Barden is a high surface area kaolin product used a filler in rubber and plastic applications.Information provided by Imerys |
|||
Particle Size | 0.30 µm | 0.30 µm | median |
Imerys Barnetâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 0.30 µm | 0.30 µm | average |
Imerys Hydrated Aluminum Silicate KT 90A-1 Kaolin KT 90A-1 is a Hydraetd Aluminum Silicate. It is a high surface area, fine particle size clay that is well suited for use as an econoMical filler.Information provided by Imerys |
|||
Particle Size | 0.30 µm | 0.30 µm | average |
Imerys Kaolexâ„¢ BN Kaolin Kaolex BN is a Hydrated Aluminum Silicate. It is an econoMical high surface area clay, well suited for use in roofing granules and refractory applications..Information provided by Imerys |
|||
Particle Size | 0.30 µm | 0.30 µm | median |
Imerys Mercapâ„¢ 100 Kaolin Information provided by Imerys |
|||
Particle Size | 0.30 - 5.0 µm | 0.30 - 5.0 µm | TEM |
Gwent Electronic Materials P2121112P1 Acid Vapor Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Particle Size | 0.30 - 5.0 µm | 0.30 - 5.0 µm | TEM |
Gwent Electronic Materials P2121112P2 Argon Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Particle Size | 0.30 - 5.0 µm | 0.30 - 5.0 µm | TEM |
Gwent Electronic Materials P2121112P4 Nitrogen Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Particle Size | 0.30 - 5.0 µm | 0.30 - 5.0 µm | TEM |
Gwent Electronic Materials P2121112P5 Ammonia Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Particle Size | 0.30 - 5.0 µm | 0.30 - 5.0 µm | TEM |
Gwent Electronic Materials P2121112P6 Oxygen Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Particle Size | 0.30 - 5.0 µm | 0.30 - 5.0 µm | TEM |
Gwent Electronic Materials P2121112P3 Tetrafluoromethane Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Particle Size | 0.30 µm | 0.30 µm | |
Shin-Etsu Silicones X-52-2265 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 0.30 - 25 µm | 0.30 - 25 µm | PSD (d<sub>50</sub> |
Terio Corporation TZY-3 Yttria Stabilized Zirconia Information provided by TERIO Corporation. |
|||
Particle Size | 0.30 - 0.50 µm | 0.30 - 0.50 µm | Planar Size |
Goodfellow HDPlas® GNP Plasma Functionalized Graphene Nanoplatelets Graphene is a carbon based material which is inherently inert and which does not like to mix with, or bond to, other materials. Its excellent properties can only be fully realized when this fundamen.. |
|||
Particle Size | 0.30 - 0.70 µm | 0.30 - 0.70 µm | |
American Elements Titanium Nanoparticles General DescriptionTitanium (Ti) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Titanium Particles are typically 10 - 80 nanometers (nm) .. |
|||
Particle Size | 0.30 - 0.60 µm | 0.30 - 0.60 µm | MA147LFE |
C.O.I.M. FILCO® 368 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Particle Size | 0.30 µm | 0.30 µm | |
Asahi Glass Fluon® XAD938 PTFE Aqueous Dispersion Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc... |
|||
Particle Size | 0.30 µm | 0.30 µm | |
Asahi Glass Fluon® AD936 PTFE Aqueous Dispersion Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc... |