Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.020 - 0.030 µm | 0.020 - 0.030 µm | outside diameter |
NanoAmor 95%, OD/ID/L: 20-30/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | outside diameter |
NanoAmor 95%, OD/ID/L: 20-40/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.030 µm | 0.020 - 0.030 µm | outside diameter |
NanoAmor 95%, OD/ID: 20-30/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | outside diameter |
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | outside diameter |
NanoAmor 95%, OD/WT/L: 20-40/5-15 nm/0.5-5 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.030 µm | 0.020 - 0.030 µm | outside diameter |
NanoAmor 95%, OD: 20-30 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.030 µm | 0.020 - 0.030 µm | outside diameter |
NanoAmor 95%, OD: 20-30 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 µm | 0.020 µm | |
Zircar Ceramics SI-RIG Silica Rigidizer Type SI-RIG Silica Rigidizer is a single part water based colloidal suspension of colloidal silica. It is principally used for rigidizing and hardening the surfaces of ZIRCAR® fibrous ceramic produ.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Antimony Nanoparticles General DescriptionAntimony (Sb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Antimony Particles are typically 20-40 nano.. |
|||
Particle Size | 0.020 - 0.080 µm | 0.020 - 0.080 µm | |
American Elements Antimony Oxide Nanopowder General DescriptionAntimony Oxide ( SbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Antimony Tin Oxide Nanoparticles General DescriptionAntimony Tin Oxide (ATO) Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. N.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Barium Titanate nanoparticles General DescriptionBarium Titanate Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nanoscale .. |
|||
Particle Size | 0.020 - 0.060 µm | 0.020 - 0.060 µm | |
American Elements Beryllium Nanoparticles General DescriptionBeryllium (Be) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Beryllium Particles are typically 20-60 nanometers (nm) with specif.. |
|||
Particle Size | 0.020 - 0.080 µm | 0.020 - 0.080 µm | |
American Elements Bismuth Oxide Nanopowder General DescriptionBismuth Oxide ( BiO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Particle Size | 0.020 - 0.10 µm | 0.020 - 0.10 µm | |
American Elements Gold Nanoparticles General DescriptionGold (Au) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Gold Particles are typically 20 - 100 nanometers (nm) with specifi.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Indium Nanoparticles General DescriptionIndium (In) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Indium Particles are typically 20-40 nanomete.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Iron Nanoparticles General DescriptionIron (Fe) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Iron Particles are typically 20-40 nanometers (.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Iron Oxide Nanopowder General DescriptionIron Oxide ( Fe2O3 and Fe3O4) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure part.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Lead Oxide Nanopowder General DescriptionLead Oxide ( PbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Lead Oxide Par.. |
|||
Particle Size | 0.020 - 0.060 µm | 0.020 - 0.060 µm | |
American Elements Magnesium Nanoparticles General DescriptionMagnesium (Mg) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Magnesium Particles are typically 20-60 nanometers (nm) with specif.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Manganese Nanoparticles General DescriptionManganese (Mn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Manganese Particles are typically 20-40 na.. |
|||
Particle Size | 0.020 - 0.080 µm | 0.020 - 0.080 µm | |
American Elements Molybdenum Oxide Nanopowder General DescriptionMolybdenum Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles... |
|||
Particle Size | 0.020 - 0.10 µm | 0.020 - 0.10 µm | |
American Elements Niobium Oxide Nanoparticles General DescriptionNiobium Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Particle Size | 0.020 - 0.10 µm | 0.020 - 0.10 µm | |
American Elements Rhenium Nanoparticles General DescriptionRhenium (Re) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Rhenium Particles are typically 20 - 100 nanometers (nm) with s.. |
|||
Particle Size | 0.020 - 0.10 µm | 0.020 - 0.10 µm | |
American Elements Ruthenium Nanoparticles General DescriptionRuthenium (Ru) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Ruthenium Particles are typically 20 - 100 nanometers (nm) wi.. |
|||
Particle Size | 0.020 - 0.080 µm | 0.020 - 0.080 µm | |
American Elements Tantalum Oxide Nanopowder General DescriptionTantalum Oxide ( TaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Tin Oxide Nanopowder General DescriptionTin Oxide ( SnO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide Parti.. |
|||
Particle Size | 0.020 - 0.080 µm | 0.020 - 0.080 µm | |
American Elements Calcium Oxide Nanopowder General DescriptionCalcium Oxide ( CaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Particle Size | 0.020 - 0.060 µm | 0.020 - 0.060 µm | |
American Elements Cobalt Nanoparticles General DescriptionCobalt (Co) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Cobalt Particles are typically 20-60 nanometers (nm) with specific sur.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Cobalt Iron Nanopowder General DescriptionCobalt Iron ( CoFe) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties.. |