Particle Size 22 - 26 µm
22 - 26 µm
10%
H.C. Starck Amperit® 519.088 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
Particle Size 22 - 26 µm
22 - 26 µm
10%
H.C. Starck Amperit® 526.088 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
Particle Size 22 - 26 µm
22 - 26 µm
10%
H.C. Starck Amperit® 527.088 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17
Particle Size 22 - 26 µm
22 - 26 µm
10%
H.C. Starck Amperit® 588.088 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 53/20 µm
Particle Size 22 - 26 µm
22 - 26 µm
10%
H.C. Starck Amperit® 547.074 Tungsten Carbide-Nickel 88-12 (WC-Ni)
Particle Size 24 - 26 µm
24 - 26 µm
D50
Sinotek Materials ZSG-25 Spherical Graphite
Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification..