Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 8.0 µm | 8.0 µm | median; Microtrac |
Nyco 400 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | >= 8.0 µm | >= 8.0 µm | 10% smaller than |
Nyco NYGLOS® 20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 8.0 µm | 8.0 µm | Median Grain Diameter |
Nabaltec APYRAL® 24 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Particle Size | 8.0 - 13 µm | 8.0 - 13 µm | d50 |
Magyar Aluminum ALOLT 38AF Aluminum Hydroxide Ground type |
|||
Particle Size | 8.0 - 11 µm | 8.0 - 11 µm | Mean particle size is 8 to 11 µm. Crystal size is 8 µm. %-325 mesh is 99.9%. |
Momentive Performance Materials HCPL Boron Nitride (BN) Powder All Grade HCP powders are high purity, fine (99%, -325 mesh), hexagonal Boron Nitride (BN). All exhibit the unique properties of BN in a form readily used in many advanced materials and processes. .. |
|||
Particle Size | 8.0 - 14 µm | 8.0 - 14 µm | average |
Momentive Performance Materials PolarTherm® PT120 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Particle Size | 8.0 - 12 µm | 8.0 - 12 µm | 10% |
H.C. Starck Amperit® 519.059 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | 90% less than |
H.C. Starck Grade A Yttrium Oxide Sintering additive for Si3N4 and AlNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | 90% less than |
H.C. Starck Grade AT Yttrium Oxide Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | 90% less than |
H.C. Starck Grade B Zirconium Carbide, ZrC Additive for hard metalsAdditive for powder metallurgyModerator in solid fuel propellant |
|||
Particle Size | 8.0 µm | 8.0 µm | 50% of particles, (VEG Powder) |
Ferro EG 2928 Glaze and Sealant Glass Glass Type: Pb-Zn-B Typical Powder Form: VEG, MVG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective an.. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | 23% |
SGL Carbon Group CF 1135 Carbon Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | 26% |
SGL Carbon Group CF 270 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | 31% |
SGL Carbon Group CF 3100 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | 13% |
SGL Carbon Group CF 480 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | 8.0 µm | 8.0 µm | Before Conversion |
Silberline Silvet® 330-20-E Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatible with.. |
|||
Particle Size | 8.0 µm | 8.0 µm | |
Silberline Silvex® 335-20-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 8.0 µm | 8.0 µm | |
Silberline SparkleBriteâ„¢ 320NL-PA SparkleBriteâ„¢ pigments are non-leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on cornflake geometry and produce strong metallic effects in solvent and wate.. |
|||
Particle Size | 8.0 - 12 µm | 8.0 - 12 µm | d90, Guaranteed |
TIMCAL TIMREX® C-LUB 304 Primary Synthetic Graphite Information provided by TIMCAL |
|||
Particle Size | 8.0 µm | 8.0 µm | d50 |
TIMCAL TIMREX® KS15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 8.0 µm | 8.0 µm | D90 (Malvern) Size E |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 8.0 µm | 8.0 µm | D90 (Malvern) Size E |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 8.0 µm | 8.0 µm | Median |
Excalibar ExBar™ W 400 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Particle Size | <= 8.0 µm | <= 8.0 µm | Max |
CIMBAR CIMBAR™ EX Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |
|||
Particle Size | 8.0 - 17 µm | 8.0 - 17 µm | For Median |
CIMBAR Crescent 12 Calcium Carbonate (CaCO3), Fine Powder CIMBAR's Crescent product line is a natural calcium carbonate ground to various particle size distributions. The crystalline structure of the calcium carbonate in Crescent products has a predominan.. |
|||
Particle Size | 8.0 µm | 8.0 µm | @ 90% |
CIMBAR MV 603 Talc MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla.. |
|||
Particle Size | 8.0 - 25 µm | 8.0 - 25 µm | fiber diameter |
BCC Products BC 32 Fibrous Glass BC 32, microglass milled fibers will increase the mechanical strengths, such as impact strength, tensile strength, compressive strength, and flexural strength in plastic tooling compounds. They are .. |
|||
Particle Size | 8.0 µm | 8.0 µm | Average Diameter |
Potters Industries Conduct-O-Fil® SN08P40 Silver-coated Sub-10 micron Particles Conduct-O-Fil® conductive particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. A variety of particle shapes offers the formulator additional .. |
|||
Particle Size | 8.0 - 12 µm | 8.0 - 12 µm | 10% |
H.C. Starck Amperit® 526.059 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Particle Size | 8.0 - 12 µm | 8.0 - 12 µm | 10% |
H.C. Starck Amperit® 547.002 Tungsten Carbide-Nickel 88-12 (WC-Ni) |