Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 6.0 µm | 6.0 µm | median; Microtrac |
Nyco M3 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 6.0 µm | 6.0 µm | median; Microtrac |
Nyco NYGLOS® M3 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 6.0 µm | 6.0 µm | Median Grain Diameter |
Nabaltec APYRAL® 33 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Particle Size | 6.0 µm | 6.0 µm | Median Grain Diameter |
Nabaltec NABALOX® NO 115-71 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 6.0 µm | 6.0 µm | |
Poco Graphite CZR Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Particle Size | 6.0 µm | 6.0 µm | |
Poco Graphite SCF-2 Ion Implant Grade Graphite An economic alternative to DFP-3-2, this 5-micron material is harder than DFP-3-2 and has high strengths without reduced porosity. |
|||
Particle Size | 6.0 µm | 6.0 µm | Median Diameter |
Omya OMYACARB® 6 - PT Calcium Carbonate A dry ground calcium carbonate with intermediate and closely sized particle distribution.Applications: An ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated po.. |
|||
Particle Size | 6.0 µm | 6.0 µm | average; ISO 13321 |
3M Dyneon™ TF 9201 PTFE
(discontinued **) Low molecular weight virgin PTFE (non-degraded)Agglomerate particlesEasily deagglomerated when incorporated into other matrixesSuitable for use in food contact applications. Complies with FDE specif.. |
|||
Particle Size | 6.0 - 12 µm | 6.0 - 12 µm | d50 |
Magyar Aluminum ALO-DFM Alumina Alumina for Polishing |
|||
Particle Size | 6.0 µm | 6.0 µm | 90% |
Minelco UltraCarb LH3 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | 6.0 µm | 6.0 µm | 3rd Streak; Fineness of Grind |
Gwent Electronic Materials C2000107P3 Silver Ink Silver Ink C2000107P3 is designed as a termination for single layer PZT ceramics. After firing the film has good adhesion and solderability.The ink is in a ready to use form at a viscosity suitable.. |
|||
Particle Size | 6.0 - 9.0 µm | 6.0 - 9.0 µm | Mean |
Momentive Performance Materials HCPH Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powders of grades HCP, HCPH, HCPL, and AC6004 are generally single-crystal hexagonal platelets with very high purity. The mean particle sizes for these ultra-.. |
|||
Particle Size | 6.0 - 23 µm | 6.0 - 23 µm | d50 |
Indium Corp. In2O3 Type A Indium Oxide, Crystalline Powder Indium Sesquioxide is a yellow colored powder. It is a stable ceramic-like material, insoluble in water and volatizes at 850°C. Indium sesquioxide is a n-type semiconductor and as such is used .. |
|||
Particle Size | <= 6.0 µm | <= 6.0 µm | 90% less than |
H.C. Starck Grade B Zirconium Diboride, ZrB2 Hot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous metalsCeramic shapes to be used in productio.. |
|||
Particle Size | 6.0 µm | 6.0 µm | Average Crystal Size - Thin Section Test |
CoorsTek AD-85 Alumina (nom. 85% Al2O3) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Particle Size | 6.0 µm | 6.0 µm | Average Crystal Size; THIN-SECTION |
CoorsTek AD-996 99.6% Alumina |
|||
Particle Size | 6.0 µm | 6.0 µm | Average Crystal Size - Thin Section Test |
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Particle Size | 6.0 µm | 6.0 µm | Average Crystal Size - Thin Section Test |
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Particle Size | 6.0 µm | 6.0 µm | Thin Section Crystal Size |
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Particle Size | 6.0 µm | 6.0 µm | < 30 wt% below (equivalent spherical diameter) |
Excalibar NewBar™ API Barite BaSO4 Powder NewBar™ API barite product is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas explorati.. |
|||
Particle Size | 6.0 µm | 6.0 µm | |
DayGlo Phantom IPO-13 Invisible Pigment, Red These materials have a yellowish or white color body under visible light and produce a bright vibrant color when exposed to an Ultra-Violet light source. Phantom pigments can be used for security an.. |
|||
Particle Size | 6.0 µm | 6.0 µm | 30% less than 6 microns |
CIMBAR BARA 200 Barium Sulfate (BaSO4) BARA 200 is a natural barium sulfate. Cimbar's BARA 200 is designed to meet all the requirements of drilling grade barite. Bara meets or exceeds all API requirements. These properties make BARA 2.. |
|||
Particle Size | <= 6.0 µm | <= 6.0 µm | 50% |
BYK Cloisite® 10A Nanoclay Cloisite® 10A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.
Information provided by Southern Clay ProductsSouthern Clay P.. |
|||
Particle Size | <= 6.0 µm | <= 6.0 µm | 50% |
BYK Cloisite® 15A Nanoclay Cloisite® 15A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Particle Size | 6.0 - 9.0 µm | 6.0 - 9.0 µm | D(0.5) |
Akzo Nobel Expancel® 461 WU 20 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 6.0 - 9.0 µm | 6.0 - 9.0 µm | D(0.5) |
Akzo Nobel Expancel® 551 DU 20 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 6.0 - 10 µm | 6.0 - 10 µm | Mean particle size |
Carborundum CarboTherm™ CTF10 Boron Nitride Powder Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect.. |
|||
Particle Size | 6.0 - 12 µm | 6.0 - 12 µm | average |
Momentive Performance Materials PolarTherm® PT160 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |
|||
Particle Size | <= 6.0 µm | <= 6.0 µm | 50% |
BYK Cloisite® Na+ Nanoclay Cloisite® Na+ is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |