Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 4.0 µm | 4.0 µm | median; Microtrac |
Nyco 10 AS WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 4.0 µm | 4.0 µm | median; Microtrac |
Nyco 10 WOLLASTOCOAT® Wollastonite Chemically treated grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Particle Size | >= 4.0 µm | >= 4.0 µm | 10% smaller than |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 4.0 µm | 4.0 µm | Median Grain Diameter |
Nabaltec NABALOX® NO 115-25 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 4.0 µm | 4.0 µm | Average Diameter |
Potters Industries Conduct-O-Fil® SC04P10 Silver-coated Sub-10 micron Particles Applications include conductive inks, conductive adhesives, partial replacement of pure silver powder. Features good conductivity, possible blends/ replacement of 100% pure silver, silver/glass has.. |
|||
Particle Size | 4.0 µm | 4.0 µm | mean aggregate size |
NanoScale NanoActive® Calcium Oxide NanoActive CaO is produced using proprietary processes to obtain high specific surface area (over 20 m²/g vs. 1-2 m²/g for standard CaO) with strong affinity towards carbon dioxide and hydrogen su.. |
|||
Particle Size | 4.0 µm | 4.0 µm | mean aggregate size |
NanoScale NanoActive® Zinc Oxide NanoActive ZnO is produced using proprietary processes to obtain high specific surface area, small crystallite size material that can be dispersed in various carrier fluids with significantly reduce.. |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | |
Poco Graphite EDM-4 EDM Graphite POCO's EDM-4 is our premier offering in the Ultrafine classification. This highly isotropic grade combines strength with moderate hardness, yielding superior electrode fabrication characteristics. T.. |
|||
Particle Size | 4.0 µm | 4.0 µm | 10% finer than |
Potters Industries Sphericel® 110P8 Hollow Glass Spheres Description: Sphericel® 110P8 hollow glass spheres displace the same volume of resin as solid spheres of the same size, but are lighter. Using Sphericel® hollow glass spheres, plastics engineers c.. |
|||
Particle Size | 4.0 - 7.0 µm | 4.0 - 7.0 µm | d90 |
Magyar Aluminum ALO-EL-2S Alumina Reactive Alumina |
|||
Particle Size | 4.0 - 7.0 µm | 4.0 - 7.0 µm | d50 |
Magyar Aluminum ALO-G4-4G Alumina Ground Alumina |
|||
Particle Size | 4.0 µm | 4.0 µm | d50 |
Magyar Aluminum ALOLT 704 Aluminum Hydroxide Viscosity Optimized Type |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | Main Break; Fineness of Grind |
Gwent Electronic Materials C2000808D2 Silver Backlight Ink Silver Ink C2000808D2 is a high resistance ink designed for use as the heating bars and tracks on automobile backlights and other circuits on glass. It has dark color when printed and fired on floa.. |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | Main Break; Fineness of Grind |
Gwent Electronic Materials C2010829D2 Silver Ink Silver Ink C2010829D2 is a high definition silver ink for LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the market.The ink has be.. |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | 3rd Streak; Fineness of Grind |
Gwent Electronic Materials C2021031D3 Electrode Ink Electrode Ink C2021031D3 is a Silver Palladium (90/10) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form.. |
|||
Particle Size | 4.0 - 6.0 µm | 4.0 - 6.0 µm | 10% |
H.C. Starck Amperit® 140.067 Tungsten (W) HS Number: 81011000 |
|||
Particle Size | <= 4.0 µm | <= 4.0 µm | 90% less than |
H.C. Starck Grade B Yttrium Oxide Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Particle Size | 4.0 - 8.0 µm | 4.0 - 8.0 µm | D 50%; Laser Light Diffraction per ASTM C1070 |
H.C. Starck Type I Pure Molybdenum MIMP Powder Description of Product: Highly deagglomerated high purity molybdenum powder for any applications requiring the most finely deagglomerated powders like paste or metal injection molding applications... |
|||
Particle Size | 4.0 - 5.0 µm | 4.0 - 5.0 µm | Median Grain (d50) |
CeramTec Alunit® Aluminum Nitride Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its .. |
|||
Particle Size | 4.0 - 5.0 µm | 4.0 - 5.0 µm | Medium Grain (d50) |
CeramTec Alunit® HS Aluminum Nitride Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. I.. |
|||
Particle Size | 4.0 µm | 4.0 µm | D50 (Malvern) Size E |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 4.0 µm | 4.0 µm | D50 (Malvern) Size E |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 4.0 µm | 4.0 µm | Median |
Excalibar ExBar™ W 4 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Particle Size | 4.0 µm | 4.0 µm | D50 |
Dandong Taico Minerals TAICOCITE® TC12 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Particle Size | 4.0 µm | 4.0 µm | Median |
CIMBAR EliteTalc® 22 Cosmetic Talc Cimbar performance Minerals MV, LLC Talc U.S.P. Cosmetic talcs are designed specifically for cosmetic formulations. Talc is commonly used in cosmetics for its ability to bind to oils, create a mois.. |
|||
Particle Size | 4.0 - 7.0 µm | 4.0 - 7.0 µm | |
Chesterton 772 Premium Nickel Anti-Seize Compound Description: Chesterton® 772 Premium Nickel Anti-Seize Compound is formulated with ultra pure raw materials. This permits 772 Premium Nickel Anti-Seize Compound to conform to most applicable equipm.. |
|||
Particle Size | 4.0 µm | 4.0 µm | |
Astro Met AmAlOx 68 Alumina - Aluminum Oxide General Description:AmAlOx 68 alumina (Astro Met Aluminum Oxide) is a high purity 99.8% aluminum oxide (alumina) ceramic which has been developed and optimized for maximum wear resistance and corros.. |
|||
Particle Size | 4.0 - 7.0 µm | 4.0 - 7.0 µm | |
Chesterton 710 Anti-Seize Compound Description: Chesterton® 710 Anti-Seize Compound is an anti-seize compound and assembly lubricant combining the high temperature, extreme pressure, and corrosion resistant properties of colloidal c.. |