Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Particle Size = 25 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 25 µm
25 µm
Median Diameter
Omya TITAN® 200 - LU Calcium Carbonate
An intermediate, dry ground calcium carbonate with a closely controlled particle size distribution.Applications: For use in latex compounds.Information supplied by Omya North America.
Particle Size 25 µm
25 µm
D<sub>50</sub>; ISO 13320-1
Victrex® PEEK 150XF Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, fine powder for compression moulding, easy flow, FDA food contact compliant, ..
Particle Size 25 µm
25 µm
ASTM D4894
3M Dyneon™ CCX1029 PTFE, 10% Carbon Fiber Filled  (discontinued **)
Type I, non-free-flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon ..
Particle Size 25 µm
25 µm
ASTM D4894
3M Dyneon™ TFM™ 1705 Modified PTFE Powder  (discontinued **)
Type II, gr. 1 PTFE. Dyneon™ TFM™ 1705 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-generat..
Particle Size 25 µm
25 µm
median
3M Dyneon™ PFA 6503 C EPC Perfluoroalkoxy Fluorothermoplastic  (discontinued **)
Dyneon PFA 6503 C EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick ..
Particle Size <= 25 µm
<= 25 µm
VWG Powder
Ferro CF 8463 Low-Temperature Sealing
VITREOUS Typical Powder Form: VSD, VWG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific..
Particle Size <= 25 µm
<= 25 µm
Ferro EG 0024 Specialty Glass
Glass Type: Si-B-MG-Al Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-ph..
Particle Size <= 25 µm
<= 25 µm
MVG Powder
Ferro EG 0225 Specialty Glass
Glass Type: MG-Al-Si (devitrified) Typical Powder Form: MVG, SRRG Typical Application: Sintering Aid / Ceramic Ferro offers a wide range of compositions for specialty applications including sinteri..
Particle Size <= 25 µm
<= 25 µm
Ferro EG 2739 Thick Film Glass
Glass Type: Pb-Zn-B Typical Powder Form: MVG Typical Application: Resistor Overglaze Ferro produces standard and custom glass products that are used in thick film compositions including resistors, ..
Particle Size <= 25 µm
<= 25 µm
Ferro EG 2782 Specialty Glass
Glass Type: Ca-Si-B Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-phase..
Particle Size <= 25 µm
<= 25 µm
Ferro EG 2783 Thick Film Glass
Glass Type: Pb-B Typical Powder Form: MVG Typical Application: Die Attachment Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct..
Particle Size <= 25 µm
<= 25 µm
RWG Powder
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to..
Particle Size 25 - 35 µm
25 - 35 µm
d50
Magyar Aluminum ALOLT 21AF Aluminum Hydroxide
Ground type
Particle Size <= 25 µm
<= 25 µm
D90
Momentive Performance Materials PolarTherm® PT100 Boron Nitride (BN) Powder
Single crystal platelet BN Powder. High aspect ratio platelets may improve thermal conductivity when used as a filler in polymers or lubricants. Features of BN include thermal conductor, electrica..
Particle Size 25 - 29 µm
25 - 29 µm
90%
H.C. Starck Amperit® 251 Gas Atomized (NiCr 80-20)
Particle Size <= 25 µm
<= 25 µm
Ferro EG 2791 Thick Film Glass
Glass Type: Bi-Pb-Zn Typical Powder Form: MVG Typical Application: End Termination Ferro produces standard and custom glass products that are used in thick film compositions including resistors, co..
Particle Size <= 25 µm
<= 25 µm
MVG Powder
Ferro EG 2928 Glaze and Sealant Glass
Glass Type: Pb-Zn-B Typical Powder Form: VEG, MVG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective an..
Particle Size <= 25 µm
<= 25 µm
Ferro IP 510 Thick Film Glass
Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto..
Particle Size <= 25 µm
<= 25 µm
RWG Powder
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to..
Particle Size 25 µm
25 µm
95%, Laser diffraction; QSOP-5&75
Shamrock Technologies MicroFLON® 1437 Thermoplastic Grade PTFE Additive
Used in high temperature engineering plastics.The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion...
Particle Size 25 µm
25 µm
Silberline Sparkle Silvex® Premier 860-20-D
Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited ..
Particle Size 25 µm
25 µm
UCAR Carbon UCAR® ATJ Isostatic Molded Graphite
Isostatically molded ATJ has been an industry standard for many years. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish. Grade ATJ has..
Particle Size 25 µm
25 µm
UCAR Carbon UCAR® ATR Isostatic Molded Graphite
Isostatically molded ATR is a lower density version of grade ATJ. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish.Typical Application..
Particle Size 25 µm
25 µm
UCAR Carbon UCAR® CGW Isostatic Molded Graphite
Isostatically molded grade CGW is an ATJ-based material that has been processed to higher density and strength. Grade CGW is characterized by low permeability, erosion resistance and surface hardnes..
Particle Size 25 µm
25 µm
D90 (Malvern) Size C
Vesta Ceramics SicoMill® Grade 4 Silicon Powder
General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu..
Particle Size <= 25 µm
<= 25 µm
Chesterton 785 Parting Lubricant
Description: Chesterton® 785 Parting Lubricant represents the newest generation of anti-seize compound. A proprietary blend of ultra-fine inorganic solid lubricants in a non-carbonizing, ashless sy..
Particle Size 25 µm
25 µm
10th%
3M A20/1000 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 25 µm
25 µm
average; ASTM D4894-98a
3M Dyneon™ TFM™ 1700 PTFE
Meets ASTM D4894 Type III, Grade 1 resinNon-free-flowing compression molding powderVery fine particle sizeDense polymer structure, low permeabilityImproved weldabilityLow deformation under loadGood ..
Particle Size 25 µm
25 µm
average; ASTM D4894-98a
3M Dyneon™ TF 1750 PTFE
Meets ASTM D4894 Type IINon-free-flowing powder gradeVery fine particle sizeGood electrical and mechanical propertiesLow molding pressureUsed in large billet moldingExcellent for production of very ..
Particle Size 25 µm
25 µm
ASTM D4894
3M Dyneon™ TFM™ 1700 Modified PTFE Powder
Type III, gr. 1 PTFE. Dyneon™ TFM™ 1700 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-genera..
Copyright © lookpolymers.com All Rights Reserved