Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 2.0 µm | >= 2.0 µm | 10% smaller than |
Nyco 400 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | >= 2.0 µm | >= 2.0 µm | 10% smaller than |
Nyco M325 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | >= 2.0 µm | >= 2.0 µm | 10% smaller than |
Nyco NYAD® 325 Wollastonite Powdered grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particl.. |
|||
Particle Size | >= 2.0 µm | >= 2.0 µm | Primary Crystal Size |
Nabaltec NABALOX® NO 115 TC Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | >= 2.0 µm | >= 2.0 µm | Primary Crystal Size |
Nabaltec NABALOX® NO 115-25 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | >= 2.0 µm | >= 2.0 µm | Primary Crystal Size |
Nabaltec NABALOX® NO 615-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | >= 2.0 µm | >= 2.0 µm | Primary Crystal Size |
Nabaltec NABALOX® NO 625-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 2.0 µm | 2.0 µm | 77% of particles less than |
Old Hickory APG-300 Kentucky Ball Clay This is an extremely low 325 Mesh wet residue clay. It can be employed in a variety of applications where high purity mineral filler is required. It has a moderate GE brightness value and is particu.. |
|||
Particle Size | 2.0 µm | 2.0 µm | Median particle diameter |
Old Hickory M&M Clays, Inc. Wilco-LPC Kaolin Clay Wilco LPC is the same selection as the SLU grade except it is in natural shredded or Airfloat (powdered) form. It offers the same benefits in a ceramic casting formulation discussed above for the SL.. |
|||
Particle Size | 2.0 µm | 2.0 µm | 50.0% of particles less than |
Old Hickory M&M Clays, Inc. Wilco-LPC Kaolin Clay Wilco LPC is the same selection as the SLU grade except it is in natural shredded or Airfloat (powdered) form. It offers the same benefits in a ceramic casting formulation discussed above for the SL.. |
|||
Particle Size | <= 2.0 µm | <= 2.0 µm | |
Hong Kun Group DBDPE Flame Retardant Chemical Name:1,2-Bis(pentabromophenyl) ethaneDecabromodiphenylethaneDecabromodiphenyl EthylCAS No. 84852-53-9All information provided by Hongkun Group |
|||
Particle Size | 2.0 - 6.0 µm | 2.0 - 6.0 µm | Primary crystal size |
Magyar Aluminum ALO-Ex35 LS Alumina Calcined Alumina |
|||
Particle Size | 2.0 - 5.0 µm | 2.0 - 5.0 µm | d50 |
Magyar Aluminum ALO-G5-4 Alumina Ground Alumina |
|||
Particle Size | >= 2.0 µm | >= 2.0 µm | 2% finer |
Malvern Minerals Novakup® L-207A Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 2.0 µm | 2.0 µm | 93% finer than |
Imerys Bardenâ„¢ Kaolin Barden is a high surface area kaolin product used a filler in rubber and plastic applications.Information provided by Imerys |
|||
Particle Size | 2.0 µm | 2.0 µm | 67% finer than |
Imerys Carverâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 2.0 µm | 2.0 µm | 89% finer than |
Imerys Hamiltonâ„¢ Kaolin Hamilton is a fine-grained kaolin with low alkali content and high PCE. These properties make for ideal air-set refractory mortars. Halloysite content provides excellent suspension and trowel abilit.. |
|||
Particle Size | 2.0 µm | 2.0 µm | 93% finer than |
Imerys Mercapâ„¢ 100 Kaolin Information provided by Imerys |
|||
Particle Size | 2.0 - 5.0 µm | 2.0 - 5.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade A Magnesium Diboride, MgB2 |
|||
Particle Size | 2.0 - 5.0 µm | 2.0 - 5.0 µm | Average |
H.C. Starck Grade A Titanium Nitride Additive for ceramic parts to increase electrical conductivityConstituent for cermets and black ceramicsRaw material for TiN sputter targets |
|||
Particle Size | 2.0 - 4.0 µm | 2.0 - 4.0 µm | Laser Diffraction D50 |
H.C. Starck Grade B Titanium Nitride Additive for ceramic parts to increase electrical conductivityConstituent for cermets and black ceramicsRaw material for TiN sputter targets |
|||
Particle Size | <= 2.0 µm | <= 2.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade B Yttrium Oxide Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Particle Size | 2.0 - 5.0 µm | 2.0 - 5.0 µm | D 50%; Laser Light Diffraction per ASTM C1070 |
H.C. Starck Type II Pure Molybdenum MIMP Powder Description of Product: Highly deagglomerated high purity molybdenum powder for any applications requiring the most finely deagglomerated powders like paste or metal injection molding applications... |
|||
Particle Size | 2.0 µm | 2.0 µm | Median |
Excalibar ExBar™ W 2 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Particle Size | 2.0 µm | 2.0 µm | D50 |
Dandong Taico Minerals TAICOCITE® TC50 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Particle Size | 2.0 µm | 2.0 µm | |
China Tungsten YG13 Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 2.0 - 4.0 µm | 2.0 - 4.0 µm | D50 |
CIMBAR UltraMag & UltraMag ST 3 Magnesium Hydroxide Powder UltraMag is a naturally ground, white, high-purity Magnesium Hydroxide suitable for a wide range of applications including water treatment slurries, plastics, rubber and flame-retardant/smoke suppre.. |
|||
Particle Size | 2.0 µm | 2.0 µm | Hegman; Grinde Gauge |
3M Dyneon™ J14 PTFE Micropowder 3M™ Dyneon™ PTFE Micropowders can be used as additives in many applications and at concentrations typically from 5 to 20%. Homogeneous incorporation is the single most important process and applic.. |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | Median Grain (d50) |
CeramTec 975 Alumina, 99.5% 975 (99.5%) offers unique technology by virtue of its optimal dispersion of the MgO phase with the alumina grains. With virtually no transgranular porosity in its microstructure, 975 exhibits high d.. |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | Median Grain (d50) |
CeramTec 977 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 977 is a zirconia toughened alumina ceramic designed for use in ballistic protection and ceramic armor. |