Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1000 - 5000 µm | 1000 - 5000 µm | |
Oceanchem Group Calcium Chloride 94-97% prills Molecular Formula: CaCl2Information Provided by Oceanchem Group |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 99-100%; ASTM D1921 |
Nitriflex NP-1021 Powdered Nitrile Smooth calendering and extrusion, low shrinkage, low die swell. Applications: hose, conveyer belt, adhesives, profilesInformation provided by Dax Resinas |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 99-100%; ASTM D1921 |
Nitriflex NP-2021 Powdered Nitrile General use for technical artifacts that require good resistance to oil and grease with good processability. Plastic modifier and impact modifier. Applications: printing blankets , flexible containe.. |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 99-100%; ASTM D1921 |
Nitriflex NP-2121 Powdered Nitrile General use for technical artifacts that require good resistance to oil and grease with good processability and transparence. Plastic modifier and impact modifier. Applications: flexible containers,.. |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 99-100%; ASTM D1921 |
Nitriflex NP-2150 Powdered Nitrile Excellent resistance to oils and fuel resistance with good mechanical properties. Applications: cement, adhesives, grouts, safe footwear, friction materials. Information provided by Dax Resinas |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 99-100%; ASTM D1921 |
Nitriflex NP-2170 Powdered Nitrile Low temperature flexibility and excellent fatigue. Applications: o-ring, gasket, hose, friction materialsInformation provided by Dax Resinas |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 99-100%; ASTM D1921 |
Nitriflex NP-2174 Powdered Nitrile Applications that require moderate chemical resistance and excellent resistance to Ozone. Applications: hose, aprons. Information provided by Dax Resinas |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 99-100%; ASTM D1921 |
Nitriflex NP-6000 Powdered Nitrile Excellent for extruded, low die swell, high tensile strength, excellent compression set properties. Applications: Printing rolls with low hardness, gaskets, blankets, rice dehusking roller, friction.. |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 99-100%; ASTM D1921 |
Nitriflex NP-6021 Powdered Nitrile Ideal for extruded products in general. Applications: rolls, printing rolls, hose tubes and cover stocks, profiles, calendared sheet for die cut gaskets, coated fabrics and mould goods.Information p.. |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 99-100%; ASTM D1921 |
Nitriflex SB-4022 Styrene Butadiene Copolymer Applications: Powdered rubber. Enables a lower mixing time and better homogenization, presenting a reduced generation of residues. Recommended for shoe soles, adhesives and seals, injected and molde.. |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 99-100%; ASTM D1921 |
Nitriflex NP-1121 Powdered Nitrile Smooth calendering and extrusion, low shrinkage, low die swell. Applications: hose, conveyer belt, adhesives.Information provided by Dax Resinas |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 99-100%; ASTM D1921 |
Nitriflex NP-2130 Powdered Nitrile High resistance to oils and fuels, associated to excellent mechanical properties. Applications: hoses, o-rings, gaskets, conveyor belts, adhesives. Information provided by Dax Resinas |
|||
Particle Size | <= 1000 µm | <= 1000 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5004 1000 Micron EVA Powder Description: ICOFLO 510-5004 is an EVA powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (inste.. |
|||
Particle Size | <= 1000 µm | <= 1000 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5005 1000 Micron EVA Powder Description: ICOFLO 510-5005 is an EVA powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (inste.. |
|||
Particle Size | <= 1000 µm | <= 1000 µm | sieve < 5% |
ICO Polymers ICOTEXâ„¢ 520-5004 1000 Micron EVA Powder Description: ICOTEX 520-5004 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and flexibility and a viny.. |
|||
Particle Size | <= 1000 µm | <= 1000 µm | sieve < 5% |
ICO Polymers ICOTEXâ„¢ 520-5005 1000 Micron EVA Powder Description: ICOTEX 520-5005 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, fast melting, great .. |
|||
Particle Size | 1000 - 20000 µm | 1000 - 20000 µm | Lumpy |
H.C. Starck Grade K1 Crystalline Boron Neutron shields and absorbers in nuclear reactorsThermistorsFilamentsPreparation of high-purity metal boridesMetallurgy (deoxidizing agent) |
|||
Particle Size | 1000 - 20000 µm | 1000 - 20000 µm | Lumpy |
H.C. Starck Grade KT 1 Crystalline Boron Neutron shields and absorbers in nuclear reactorsThermistorsFilamentsPreparation of high-purity metal boridesMetallurgy (deoxidizing agent) |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 100%; Malvern |
SABIC Innovative Plastics NORYL SA120FIN PPE Noryl* SA120FIN resin is a powder version of a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120FIN is intended for use as additive or building block in a variety of the.. |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 1; Malvern |
SABIC Innovative Plastics NORYL SA120FIN PPE (Asia Pacific) Noryl* SA120FIN resin is a powder version of a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120FIN is intended for use as additive or building block in a variety of the.. |
|||
Particle Size | <= 1000 µm | <= 1000 µm | 1; Malvern |
SABIC Innovative Plastics NORYL SA120FIN PPE (Europe-Africa-Middle East) Noryl* SA120FIN resin is a powder version of a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120FIN is intended for use as additive or building block in a variety of the.. |
|||
Particle Size | >= 1000 µm | >= 1000 µm | 10% Max; 540MA3C5E |
Solvay MIRAPOL® SURF-S 410 Surfactant Description: Granulated rinse aid polymer for use in automatic dish washing powders or tablets. 18% activeIdentification: BLEND OF ACRYLIC BASED POLYMER AND SODIUM TRIPOLYPHOSPHATE.Use level : 0.5 â.. |
|||
Particle Size | 1000 µm | 1000 µm | at a density of 2.12 g/cc |
TIMCAL TIMREX® KS150-600SP Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 1000 µm | 1000 µm | at a density of 2.12 g/cc |
TIMCAL TIMREX® KS500 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 1000 µm | 1000 µm | at a density of 2.12 g/cc |
TIMCAL TIMREX® KS5-75TT Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 1000 µm | 1000 µm | |
Zeon Chemicals Nipol® 1492P80 Nitrile Powder and Crumb Elastomer Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is .. |
|||
Particle Size | 1000 - 1700 µm | 1000 - 1700 µm | min 92%; BC HSZ 326:2001/1 screening |
BorsodChem ONGROSTYR F-III Expandable Polystyrene (EPS) ONGROSTYR F-III is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i... |
|||
Particle Size | 1000 µm | 1000 µm | at a density of 2.12 g/cc |
TIMCAL TIMREX® KS300-1250 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | >= 1000 µm | >= 1000 µm | 3 Max; 540MAC95 |
Solvay MIRAPOL® SURF-S PFREE POWER Surfactant Description: Blend of acrylic based polymer and sodium carbonate. This polymer is used as a rinse-aid agent to replace the nonionic surfactant 3-in-1 product in automatic dish wash. It is very effic.. |
|||
Particle Size | 1000 µm | 1000 µm | Median |
Eliokem Sunigum® P95 Acrylate Elastomer Outstanding heat and UV resistance. Wide range of capabilities. Crosslinked polymer structure. CaCO3 partitioning agent.Can be used in PVC, TPU, TPE/TPO and engineering plastic blends.Used in auto.. |