Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.40 µm | 0.40 µm | Median; Laser Diffraction |
Nabaltec APYRAL® 200 SM Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Particle Size | 0.40 µm | 0.40 µm | Median particle diameter |
Old Hickory APG-300 Kentucky Ball Clay This is an extremely low 325 Mesh wet residue clay. It can be employed in a variety of applications where high purity mineral filler is required. It has a moderate GE brightness value and is particu.. |
|||
Particle Size | 0.40 µm | 0.40 µm | Median Diameter |
Omya HYDROCARB® HG Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Particle Size | 0.40 µm | 0.40 µm | Crystal Size |
Momentive Performance Materials PolarTherm® PT131 Boron Nitride (BN) Powder Boron Nitride powders are produced by GE Advanced Ceramics in more than 50 individual (standard and custom) grades to meet a wide variety of application needs.For use in: Electrically insulating/the.. |
|||
Particle Size | 0.40 µm | 0.40 µm | Crystal Size |
Momentive Performance Materials PolarTherm® PT132 Boron Nitride (BN) Powder Boron Nitride powders are produced by GE Advanced Ceramics in more than 50 individual (standard and custom) grades to meet a wide variety of application needs.For use in: Electrically insulating/the.. |
|||
Particle Size | 0.40 - 0.80 µm | 0.40 - 0.80 µm | d10 |
Indium Corp. Fine ITO Indium Tin Oxide Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo.. |
|||
Particle Size | 0.40 - 25 µm | 0.40 - 25 µm | PSD (d<sub>50</sub> |
Terio Corporation TZ-1~30 Zirconia Information provided by TERIO Corporation. |
|||
Particle Size | <= 0.40 µm | <= 0.40 µm | |
Dow Corning 2-8197 EMULSION Dow Corning 2-8197 Emulsion is a non-ionic emulsion of a reactive aminofunctional polydimethylsiloxane suitable to provide a "Fabric Care" benefit for rinse cycle fabric softeners. The use of this p.. |
|||
Particle Size | 0.40 - 0.60 µm | 0.40 - 0.60 µm | |
C.O.I.M. FILCO® 352 Unsaturated Bisphenolic Polyester Polymer for Glass Fiber Sizing Description: Unsaturated Bisphenolic Polyester Polymer for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in .. |
|||
Particle Size | 0.40 µm | 0.40 µm | Grain |
CeramTec MZ BE Zirconia 3Y-TZP, Dental Grade MZ BE is a yttria-stabilized tetragonal zirconia used in dental applications. |