Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 0.0050 µm | <= 0.0050 µm | outer diameter |
NanoAmor 50% DWNT Double Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD/ID/L: 10-20/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | core diameter |
NanoAmor 95%, OD/ID/L: 10-30/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | core diameter |
NanoAmor 95%, OD/ID/L: 20-40/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD/ID/L: 50-80/5-15 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD/ID: 10-20/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD/ID: 20-30/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | core diameter |
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | core diameter |
NanoAmor 95%, OD/ID: 60-100/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | wall thickness |
NanoAmor 95%, OD/WT/L: 20-40/5-15 nm/0.5-5 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD: 10-20 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD: 20-30 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | inside diameter |
NanoAmor 95%, OD: 20-30 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD: 30-50 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD: 30-50 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD: 50-80 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.030 µm | 0.0050 - 0.030 µm | wall thickness |
NanoAmor 99%, OD/WT/L: 40-70/5-30 nm/0.5-5 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD/ID: 30-50/5-15 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.010 µm | 0.0050 - 0.010 µm | core diameter |
NanoAmor 95%, OD/ID: 40-60/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.015 µm | 0.0050 - 0.015 µm | inside diameter |
NanoAmor 95%, OD/ID: 50-80/5-15 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.0050 - 0.10 µm | 0.0050 - 0.10 µm | |
American Elements Hafnium Oxide Nanopowder General DescriptionHafnium Oxide or Hafnia Nanopowder or Nanoparticles (HfO), nanodots or nanocrystals are white high surface area particles. Nanoscale Hafnium Oxide Nanoparticles are typically 5 - .. |
|||
Particle Size | 0.0050 - 0.10 µm | 0.0050 - 0.10 µm | |
American Elements Indium Oxide Nanopowder General DescriptionIndium Oxide Nanopowder or Nanoparticles (InO), nanodots or nanocrystals are white high surface area particles. Nanoscale Indium Oxide Nanoparticles are typically 5 - 100 nanomete.. |
|||
Particle Size | 0.0050 - 0.10 µm | 0.0050 - 0.10 µm | |
American Elements Magnesium Oxide Nanopowder General DescriptionMagnesium Oxide Nanoparticles or Magnesia Nanoparticles (MgO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Magnesium Oxide Nanoparticle.. |
|||
Particle Size | 0.0050 - 0.10 µm | 0.0050 - 0.10 µm | |
American Elements Manganese Oxide Nanopowder General DescriptionManganese Oxide Nanopowder (MnO), nanodots or nanoparticles are high surface area particles. Nanoscale Manganese Oxide Nanoparticles are typically 5 - 100 nanometers (nm) with spe.. |
|||
Particle Size | 0.0050 - 0.025 µm | 0.0050 - 0.025 µm | |
American Elements Silicon Nanoparticles General DescriptionSilicon (Si) Nanoparticles, nanodots or Nanopowder are spherical high surface area metal particles. Nanoscale Silicon Particles are typically 5-25 nanometers (nm) with specific su.. |
|||
Particle Size | 0.0050 - 0.10 µm | 0.0050 - 0.10 µm | |
American Elements Silicon Oxide Nanopowder General DescriptionSilicon Oxide (SiO2) Nanopowder, Silica Nanoparticles or nanodots are high surface area particles. Nanoscale Silicon Oxide Nanoparticles or Silica Particles are typically 5 - 100 .. |
|||
Particle Size | 0.0050 - 0.10 µm | 0.0050 - 0.10 µm | |
American Elements Yttria stabilized Zirconia General DescriptionYttria stabilized Zirconia or Zirconium Oxide Nanopowder or Nanoparticles (YSZ), nanodots or nanocrystals are white high surface area particles available fully stabilized (8 mol%).. |
|||
Particle Size | 0.0050 - 0.045 µm | 0.0050 - 0.045 µm | |
American Elements Yttrium Nanoparticles General DescriptionYttrium (Y) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Yttrium Particles are typically 5 - 45 nanometers (nm) with specific s.. |
|||
Particle Size | 0.0050 - 0.10 µm | 0.0050 - 0.10 µm | |
American Elements Zirconium Oxide Nanopowder General DescriptionZirconium Oxide or Zirconia Nanopowder or Nanoparticles (ZrO2), nanodots or nanocrystals are white high surface area particles available in monoclinic or as stabilized or doped wi.. |
|||
Particle Size | 0.0050 µm | 0.0050 µm | |
Dow Corning 2-8203 SILICONE EMULSION Dow Corning 2-8203 Emulsion is an amidofunctional siloxane microemulsion suitable to provide a "Fabric Care" benefit for rinse cycle fabric softeners. The use of this product provides softness, wate.. |