Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.40 - 2.70 g/cc | 0.0867 - 0.0975 lb/in³ | |
Reade Advanced Materials Ilmenite Powder (FeTiO3) Description: A naturally mined iron titanium oxide mineral. It is generally black as sand, odorless, tasteless, opaque under a microscope, non-flammable and insoluble at 20 deg. C. Physical Properti.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS SiC 70 D GM Moldable Refractory Material Description: This gunning material is supplied as a dry powder. Curas SiC 70 D GM has a phosphate bond and is specially developed as a protection layer on boiler tubes.Remarks: The stated chemical c.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURASBOND 85 Moldable Refractory Material Description: Curasbond 85 is a pouring repairmass, characterized by excellent resistance to aluminum and rapid hardening. The product is supplied in two components: a dry powder and a liquid. It can.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 170 Dense Refractory Castable Description: A general purpose castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks: These v.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resista.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 170 M GS (R) Dense Vibrating Refractory Castable Description: Vibron 170 M GS (R) is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sl.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS SiC 70 D Moldable Refractory Material Description: This material is supplied as a dry powder and has to be mixed with clean potable water to the necessary consistency. Curas SiC 70D has a phosphate bond and is specially developed for b.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 170 M RAPID Dense Vibrating Refractory Castable Description: Vibron 170 M Rapid is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sla.. |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | |
Chosun Refractories BP-95A Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | |
Chosun Refractories CUN-804 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.60 - 2.70 g/cc | 0.0939 - 0.0975 lb/in³ | |
China-Yixing Longly Refractories Slab SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |
|||
Bulk Density | 2.55 - 2.70 g/cc | 0.0921 - 0.0975 lb/in³ | |
China-Yixing Longly Refractories Tube SiC SiC tube made by our company have lots of superior performance, such as high refractoriness, good wear and corrosion resistance, hardness, strength, thermal conductivity, thermal shock stability, as.. |