Physical Properties Metric English Comments
Bulk Density 2.20 - 2.30 g/cc
0.0795 - 0.0831 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 50 PD Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre..
Bulk Density 2.20 - 2.30 g/cc
0.0795 - 0.0831 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 60 S Moldable Refractory Material
Description: Because this material contains a high percentage of sillimanite, it has a very good thermal shock resistance together with a very good slag resistance. Therefore this material finds its..
Bulk Density 2.20 - 2.30 g/cc
0.0795 - 0.0831 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 160 HF Dense Refractory Castable
Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the ..
Bulk Density 2.20 - 2.30 g/cc
0.0795 - 0.0831 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 50 D Moldable Refractory Material
Description: Because of special additions this moldable already has a reasonable strength at room temperature. This material is supplied as a dry powder, it has to be mixed with potable water to the..
Bulk Density 2.10 - 2.30 g/cc
0.0759 - 0.0831 lb/in³
China-Yixing Longly Refractories Cordierite Ceramics (Heat Resistance Ceramics)
LONGLY's cordierite ceramics' main crystal phrase is 2MgO-2Al2O2-5SiO2, this composition has low thermal expansion coefficient and excellent thermal shock resistance. Maximum service temperature is..
Bulk Density 2.10 - 2.30 g/cc
0.0759 - 0.0831 lb/in³
China-Yixing Longly Refractories 75 Alumina Ceramic