Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.801 - 0.897 g/cc | 0.0289 - 0.0324 lb/in³ | Loose |
KaMin KaMin® HG Kaolin Clay - Waterwashed KaMin® HG is an economical, general purpose, water-washed kaolin with fine particle size and intermediate brightness. It is suitable for water borne paint, ink and adhesive applications.Industry:.. |
|||
Bulk Density | 0.801 - 0.897 g/cc | 0.0289 - 0.0324 lb/in³ | Loose |
KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness KaMin® HG90 is a high brightness, ultra-fine particle size, platy kaolin with moderate water demand providing good tinting strength, Ti02 extension and gloss in water based paints. KaMin® HG90.. |
|||
Bulk Density | 0.801 - 0.897 g/cc | 0.0289 - 0.0324 lb/in³ | Loose |
KaMin KaMin® Tek 2001 Clay The uniform, narrow particle size distribution and excellent color makes Kamin® TEK 2001 the preferred extender for gloss latex paints where optimum TiO2 spacing is desired without adverse effect.. |
|||
Bulk Density | 0.801 - 0.897 g/cc | 0.0289 - 0.0324 lb/in³ | Loose |
KaMin Polyfil® HG Kaolin Clay - Waterwashed Polyfil® HG is an ultra-fine particle size, moderate brightness water washed kaolin clay. It offers acid resistance, barrier properties, reinforcement, neutral ph, and extremely low crystalline .. |
|||
Bulk Density | 0.801 - 0.897 g/cc | 0.0289 - 0.0324 lb/in³ | Loose |
KaMin Polyfil® HG90 Kaolin Clay - Waterwashed High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R.. |