Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | |
Raschig Group PiMC 1221 High gloss PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | |
Raschig Group PiMC 1249 Sanitary, mix color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | |
Raschig Group PiMC 1253 Highly flame retardant This FR PiMC grade has been developed for top coats over M1 SMC/BMC grades. Such combinations will meet Europe’s most stringent FR tests for interiors of rolling stock, such as BS 476 and Spanish E.. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | |
Raschig Group PiMC 1841 Metallic colors Adding metallic effect pigments to powder coatings gave rise to several application problems such as “spitting”. Synres-Almoco’s Metallic PiMC 1841 ensures easy processing and homogeneous surface.. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | |
Raschig Group PiMC 1949 Granite colors PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | DIN 53 468 |
Perstorp Compounds Aminel FX Melamine Organically reinforced melamine material with excellent flow properties and high flexibility suitable for applications involving high complexity and surface demands.Information provided by Perstorp .. |
|||
Bulk Density | 0.500 - 0.700 g/cc | 0.0181 - 0.0253 lb/in³ | |
Solvay Chemicals Ixper® 25M Magnesium Peroxide IXPER® 25M is a Magnesium Peroxide powder used in a wide range of applications in environmental, and oil drilling e.g. markets. EINECS Number: 215-627-7/CAS Number: 1335-26-8Information provided .. |
|||
Bulk Density | 0.600 - 0.700 g/cc | 0.0217 - 0.0253 lb/in³ | Powder Density; ISO 60 |
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit,.. |