Physical Properties Metric English Comments
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9212 E Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9216 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9612 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9620 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9622 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9816 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 - 1.35 g/cc
0.0452 - 0.0488 lb/in³
Nabaltec GRANALOX® NM 9923 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.25 g/cc
0.0452 lb/in³
Dried at 110°C
Sharadaa Ceramics REFINSUL 11 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Bulk Density 1.25 g/cc
0.0452 lb/in³
Dried at 110°C
Sharadaa Ceramics REFINSUL 11LI Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Bulk Density >= 1.25 g/cc
>= 0.0452 lb/in³
After Drying at 110°C
Sharadaa Ceramics ZAP 013 Smart Cast Application
Special Properties: Low Density, High Strength, Low Thermal ConductivityIndustry: Multi PurposeApplication: All type furnaces as a back up layer, Insulating Burner BlocksInformation provided by Shar..
Bulk Density >= 1.25 g/cc
>= 0.0452 lb/in³
Chosun Refractories C-3 Insulating Firebrick