Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | Loose |
Nyco NYGLOS® M50 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 1.20 - 1.30 g/cc | 0.0434 - 0.0470 lb/in³ | |
Nabaltec GRANALOX® NM 9212 F Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.20 - 1.35 g/cc | 0.0434 - 0.0488 lb/in³ | |
Nabaltec GRANALOX® NM 9510 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D4894 |
3M Dyneon™ CC646/S Custom Compound
(discontinued **) This compound consists of a mixture of 60% bronze blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Bulk Density | 1.20 - 1.30 g/cc | 0.0434 - 0.0470 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 110 Refractory Insulating Castable Description: Golite 110 is composed of a light weight refractory aggregate plus several additives to improve the mechanical and refractory properties.Remarks: These values apply to cast products. Al.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0179 Borosilicate Glass Spheres Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0179 beads include: calibration, high temperature spacer material for gauge control,.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0186 Borosilicate Glass Spheres Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0186 beads include: high temperature spacer material for gauge control, coating, fil.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0263 Cu Coated Borosilicate Glass Spheres Appearance: Solid borosilicate glass microspheres with metallic copper coatingTypical applications of GL-0263 glass microspheres include: conductive filler for plastic, pigment, and etc.Information .. |
|||
Bulk Density | 1.20 - 1.80 g/cc | 0.0434 - 0.0650 lb/in³ | loose |
Solvay Chemicals Barium carbonate coarse powder Barium carbonate coarse powder is used for the production of display glass, crystal glass and other special glass, glazes, frits and enamels. Barium carbonate coarse powder is also used in the ferri.. |
|||
Bulk Density | <= 1.20 g/cc | <= 0.0434 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL ZAP-017 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Bulk Density | <= 1.20 g/cc | <= 0.0434 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL ZAP-018 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | Loose |
Excalibar ExBar™ 400 Barite BaSO4 Powder ExBar™ industrial barytes products are manufactured from a high-quality natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, plastics, rubber, .. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | Packed |
Excalibar ExCal® 325 Calcium Carbonate CaCO3 Powder ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other appli.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-201SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Good fluidity, suited to making moldings of complex shapes, requiring high fluidity.Information provided by Daikin Industries. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-210AS PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-211SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Tubing and injection molded parts requiring high stress crack resistance, etc.Information provided by Daikin Industries. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-221SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-230ASL PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for extrusion molded parts. Piping, tube, etc... |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON NP-101 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON NP-120 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON NP-130 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
Bulk Density | >= 1.20 g/cc | >= 0.0434 lb/in³ | |
Chosun Refractories C-2 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Chosun Refractories LWB-120 Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | Tapped |
CIMBAR EliteTalc® 20 Cosmetic Talc Cimbar performance Minerals MV, LLC Talc U.S.P. Cosmetic talcs are designed specifically for cosmetic formulations. Talc is commonly used in cosmetics for its ability to bind to oils, create a mois.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-210 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Injection molded parts, wire insulation, etc.Information provided .. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-230 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON AP-231SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |
|||
Bulk Density | 1.20 g/cc | 0.0434 lb/in³ | |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |