Physical Properties Metric English Comments
Bulk Density 1.10 g/cc
0.0397 lb/in³
Tapped
Nyco NYAD® 400 Wollastonite
Chemically treated powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Loose
Nyco NYAD® M100 Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Tapped
Nyco NYAD® M325 Wollastonite
Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Tapped
Nyco NYAD® MD325 Wollastonite
Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Tapped
Nyco NYGLOS® MSTPO Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Bulk Density 1.10 - 1.20 g/cc
0.0397 - 0.0434 lb/in³
Nabaltec GRANALOX® NM 9916 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.10 - 1.30 g/cc
0.0397 - 0.0470 lb/in³
Nabaltec NABALOX® NO 625-31 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Nabaltec NABALOX® NO 635 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Nabaltec NABALOX® NO 645 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Packed
Omya SNOWHITE® 3 - PT Calcium Carbonate
A dry ground calcium carbonate with excellent fineness, color, and dispersion characteristics.Applications: Employed in rubber and plastic applications such as rigid PVC and plasticized PVC. Also us..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Zircar Zirconia HfF-15 Hafnia Knit Textile Insulation
Our hafnia (HfO2) fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-stabilized zirconia cloths and felts. Our high purity hafnia fiber and textiles are off..
Bulk Density 1.10 g/cc
0.0397 lb/in³
ASTM D4894
3M Dyneon™ CC655 PTFE, 50% Stainless Steel Filled  (discontinued **)
Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div..
Bulk Density 1.10 - 1.20 g/cc
0.0397 - 0.0434 lb/in³
Inhance Fluoro-Seal INHANCE® Ti-9000 Titanium Carbide
Product Description: INHANCE Ti-9000 consists of spherically shaped titanium carbide micro grains. This product is used to make other INHANCE polymer alloys. When incorporated in polymers, unique ..
Bulk Density 1.10 - 1.20 g/cc
0.0397 - 0.0434 lb/in³
Inhance Fluoro-Seal INHANCE® Ti-9100 Titanium Carbide Polymer Alloy
Product Description: INHANCE Ti-9100 polymer alloy consists of spherically shaped titanium carbide micro grains coated with a thin layer of a proprietary coupling agent. This product was designed ..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Tap Density
Momentive Performance Materials HCR48 Boron Nitride (BN) Powder
GE Advanced Ceramics boron nitride (BN) powder grades HCR48, HCJ48, and HCM are large, high-density agglomerates, of ~10 µm crystals, with average particle sizes between 175-275 µm and tap den..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Sharadaa Ceramics 29 Insulation Bricks-ASTM
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Sharadaa Ceramics HF 60 AL Insulation Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Dried at 110°C
Sharadaa Ceramics REFINSUL 9 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Sharadaa Ceramics HFK Insulation Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Bulk Density <= 1.10 g/cc
<= 0.0397 lb/in³
Dried at 110°C
Sharadaa Ceramics REFINSUL ZAP-016 Insulating Castables
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Size C (tapped)
Vesta Ceramics SicoMill® Grade 2 Silicon Powder
General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Size C (tapped)
Vesta Ceramics SicoMill® Grade 4 Silicon Powder
General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Zircar Zirconia HfF-15 Hafnia Knit Textile Insulation
Our hafnia (HfO2) fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-stabilized zirconia cloths and felts. Our high purity hafnia fiber and textiles are off..
Bulk Density 1.10 g/cc
0.0397 lb/in³
DuPont™ Nomex® 410 Paper, 30 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Bulk Density 1.10 g/cc
0.0397 lb/in³
Daikin NEOFLON M-300P PCTFE Pellets
NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Pellets.Processing Methods: Extrusion.Uses: Rods, small parts.Information provided by Daikin Industries.
Bulk Density >= 1.10 g/cc
>= 0.0397 lb/in³
Chosun Refractories C-1 Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density >= 1.10 g/cc
>= 0.0397 lb/in³
Chosun Refractories HL-16 Special Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 1.10 g/cc
0.0397 lb/in³
Dispersion; ASTM D1298
3M Dyneon™ PFA 6910GZ Fluoroplastic Dispersion
3M™ Dyneon™ PFA 6910GZ is a 50% solids fluorothermoplastic aqueous dispersion. It is a copolymer of tetrafluoroethylene and perfluorinated comonomers, with a melt viscosity several orders of magni..