Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | Tapped |
Nyco NYAD® M400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | Tapped |
Nyco NYAD® MD400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Bulk Density | 1.00 - 1.10 g/cc | 0.0361 - 0.0397 lb/in³ | |
Nabaltec GRANALOX® NM 9922 I Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Bulk Density | 1.00 - 1.20 g/cc | 0.0361 - 0.0434 lb/in³ | |
Nabaltec NABALOX® NO 615-30 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 1.00 - 1.20 g/cc | 0.0361 - 0.0434 lb/in³ | |
Nabaltec NABALOX® NO 625-30 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | <= 1.00 g/cc | <= 0.0361 lb/in³ | |
Magyar Aluminum ALOLT 28AF Aluminum Hydroxide Ground type |
|||
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | |
MarkeTech Repton 601 Mullite Brand 601 features: High porosity-low bulk density.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, e.. |
|||
Bulk Density | <= 1.00 g/cc | <= 0.0361 lb/in³ | Tap density |
Indium Corp. 4N Indium Acetate Indium Acetate is a white powder. It is freely soluble in mineral acid and acetic acid, and exhibits an acetic smell. Its particles are needle-shaped and it decomposes to indium oxide upon heating.. |
|||
Bulk Density | <= 1.00 g/cc | <= 0.0361 lb/in³ | Tap density |
Indium Corp. 5N Indium Acetate Indium Acetate is a white powder. It is freely soluble in mineral acid and acetic acid, and exhibits an acetic smell. Its particles are needle-shaped and it decomposes to indium oxide upon heating.. |
|||
Bulk Density | 1.00 - 1.10 g/cc | 0.0361 - 0.0397 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 1.2.4. Mix Refractory Insulating Castable Description: This lightweight castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Remarks: Th.. |
|||
Bulk Density | 1.00 - 1.10 g/cc | 0.0361 - 0.0397 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va.. |
|||
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | Standard; Graphite |
GrafTech GRAFOIL® GHN Standard Fluid Sealing Laminate, Non-Metal Reinforced GRAFOIL® Grade GHN is an unbranded laminate made with GRAFOIL® Grade TG-337 flexible graphite, thermally bonded to both faces of a plastic insert. It is not certified to any industry standards.. |
|||
Bulk Density | 1.00 - 2.00 g/cc | 0.0361 - 0.0723 lb/in³ | tapped |
Solvay Chemicals Barium carbonate standard powder Barium carbonate standard powder is used in the production of special glass, glazes, brick and tile industry, ceramic and ferrite industry. Barium carbonate standard powder is also used for removing.. |
|||
Bulk Density | 1.00 - 1.60 g/cc | 0.0361 - 0.0578 lb/in³ | loose |
Solvay Chemicals Strontium carbonate coarse powder Strontium carbonate coarse powder is used in the production of glazes, frits and for production of strontium pigments. Another application for strontium carbonate coarse powder is the production of .. |
|||
Bulk Density | 1.00 g/cc @Temperature 200 °C |
0.0361 lb/in³ @Temperature 392 °F |
|
Sharadaa Ceramics Sharada LTM 1.0 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | >= 1.00 g/cc | >= 0.0361 lb/in³ | Tap Density |
Sinotek Materials ZSG-15 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Bulk Density | 1.00 - 1.20 g/cc | 0.0361 - 0.0434 lb/in³ | 540MA3C63 |
Solvay MIRAPOL® SURF-S 411 HA Surfactant Description: Rinse aid polymer specially formulated for auto dish wash powders and tablets. Recommended as a substitute to rinse aid surfactants. Enables raw material cost saving, while boosting rin.. |
|||
Bulk Density | >= 1.00 g/cc | >= 0.0361 lb/in³ | Tap Density |
Sinotek Materials ZSG-17 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Bulk Density | >= 1.00 g/cc | >= 0.0361 lb/in³ | Tap Density |
Sinotek Materials ZSG-20 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | Size B (apparent) |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | Size B (apparent) |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 60 |
Vyncolit X659 Glass, Mineral and Graphite Filled Novolac Phenolic Novolac resin based, glass fiber, mineral and graphite filled. Grade with superior stiffness, high dimensional stability and excellent tribological properties. Good chemical resistance against sever.. |
|||
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | |
Dow Corning SYL-OFF® PMCPSL 8 Crosslinker Syl-Off SL 8 Crosslinker is very fast cure (contains mist reduction additive)Information provided by Dow Corning |
|||
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | |
Dow Corning SYL-OFF® PMCPSL 9176 Anchorage Additive Syl-Off® SL 9176 Anchorage Additive is one component of a multi-component silicone release system designing for coating on film substrates.Information provided by Dow Corning |
|||
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | |
DuPont™ Nomex® 410 Paper, 12 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | |
Daikin NEOFLON EP-610 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | |
Daikin NEOFLON EP-610AS ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Bulk Density | >= 1.00 g/cc | >= 0.0361 lb/in³ | |
Chosun Refractories HL-15 Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 1.00 g/cc | 0.0361 lb/in³ | |
Daikin NEOFLON EP-541 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Bulk Density | >= 1.00 g/cc | >= 0.0361 lb/in³ | Tap Density |
Sinotek Materials ZSG-25 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |