Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | Loose |
Nyco M1250 AS WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | Loose |
Nyco M1250 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | Loose |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | Loose |
Nyco MD1250 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.721 g/cc | 0.0260 lb/in³ | Tapped |
Nyco NYAD® G Special Wollastonite Wollastonite (calcium metasilicate, or CaSiO3) is a naturally occurring white, non-metallic mineral with an acicular or needle-shaped crystal structure. This distinctive property makes wollastonite .. |
|||
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | ASTM D 792 |
NOVA Chemicals Sclair® 72A Butene Copolymer LLDPE Injection Molding Resin 72A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. 72A is su.. |
|||
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | ASTM D4894 |
3M Dyneon™ CC603 PTFE, 15% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | ASTM D4745 |
3M Dyneon™ CC603 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 15% fiberglass blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Bulk Density | 0.721 g/cc | 0.0260 lb/in³ | loose |
Imerys Minsparâ„¢ 3 Ground Feldspar Minsparâ„¢ 3 is a coarse particle size, ground Feldspar with a tightly controlled particle size distribution. The angular particle shape and inherent cheMical resistance make Minsparâ„¢ 3 an e.. |
|||
Bulk Density | 0.721 - 0.753 g/cc | 0.0260 - 0.0272 lb/in³ | Aggregate, dried, 6 x 14 mesh |
St. Cloud Natural Zeolite (Clinoptilolite) Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large inter.. |
|||
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | ASTM D1895 |
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | ASTM D1895 |
Plenco 3303 Phenolic, Granular, Compression Molded Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b.. |
|||
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | ASTM D1895 |
Plenco 4300 Phenolic, Granular, Compression Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | ASTM D1895 |
Plenco 6500 Phenolic, Briquette, Injection Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | |
DuPont™ Nomex® 410 Paper, 2 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Bulk Density | 0.721 g/cc | 0.0260 lb/in³ | Tapped |
CIMBAR CIMTUFF® 9103 Talc CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® .. |
|||
Bulk Density | 0.721 g/cc | 0.0260 lb/in³ | Tapped |
CIMBAR CIMTUFF® 9103s Talc CIMTUFF® 9103s talc is a treated talc produced from high purity ore, which provides low iron content, low surface area and superior color in dry form as well as when incorporated with resins. CIMT.. |
|||
Bulk Density | 0.721 g/cc | 0.0260 lb/in³ | Tapped |
CIMBAR CLEAR-BLOC® 80 Antiblock Talc CLEAR-BLOC® 80 talc, produced from high purity ore provides high brightness, clarity, low iron content and low surface area for primary use as an anti-block additive in LDPE and LLDPE film applicat.. |
|||
Bulk Density | 0.721 g/cc | 0.0260 lb/in³ | Tapped |
CIMBAR MV 603 Talc MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla.. |
|||
Bulk Density | 0.721 - 0.801 g/cc | 0.0260 - 0.0289 lb/in³ | Dow Method |
Dow Saran® 168 Information provided by Dow |
|||
Bulk Density | 0.721 - 0.801 g/cc | 0.0260 - 0.0289 lb/in³ | Dow Method |
Dow Saran® 2032 Information provided by Dow |
|||
Bulk Density | 0.720 g/cc | 0.0260 lb/in³ | Tap |
TIMCAL TIMREX® KS300-1250 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |