Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.680 g/cc | 0.0246 lb/in³ | |
Zircar Zirconia ZYK-15 Zirconia Cloth Insulation Zirconia Cloth Type ZYK-15 is a tricot knit cloth nominally 0.012” thick composed of yttria stabilized zirconia fibers. This material offers extreme temperature and chemical resistance in a flexibl.. |
|||
Bulk Density | 0.680 g/cc | 0.0246 lb/in³ | ASTM D1895 |
Plenco 1501 Polyester, Briquette, Compression Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Bulk Density | 0.680 g/cc | 0.0246 lb/in³ | ASTM D1895 |
Plenco 3356 Phenolic, Granular, Compression Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Bulk Density | 0.680 g/cc | 0.0246 lb/in³ | ASTM D1895 |
Plenco 4304 Phenolic, Nodular, Transfer Molded PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component .. |
|||
Bulk Density | 0.680 g/cc | 0.0246 lb/in³ | ASTM D1895 |
Plenco 4327 Phenolic, Granular, Compression Molded PLENCO 04327 is a heat resistant mineral filled phenolic molding compound offering excellent cosmetic characteristics and improved heat resistant properties. PLENCO 04327 is not intended for electri.. |
|||
Bulk Density | 0.680 g/cc | 0.0246 lb/in³ | |
Zircar Zirconia ZYK-15 Zirconia Cloth Insulation Zirconia Cloth Type ZYK-15 is a tricot knit cloth nominally 0.012” thick composed of yttria stabilized zirconia fibers. This material offers extreme temperature and chemical resistance in a flexibl.. |
|||
Bulk Density | 0.680 g/cc | 0.0246 lb/in³ | ASTM D1895 |
Plenco 4002 Phenolic, Granular, Injection Molded PLENCO 04002 is a heat resistant, mineral filled phenolic molding compound offering excellent mechanical strength and dimensional stability at elevated temperatures. UL recognized under component fi.. |
|||
Bulk Density | 0.680 g/cc | 0.0246 lb/in³ | ASTM D1895 |
Plenco 4311 Phenolic, Granular, Compression Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Bulk Density | 0.680 g/cc | 0.0246 lb/in³ | |
DuPont™ Nomex® E56 Paper, 7 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |