Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | |
Imerys PLM 3 Ground Mica PLM 3 is a dry Ground Mica (complex potassium aluminum silicate) with a controlled size distribution.Information provided by Imerys |
|||
Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | DIN 53466 |
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | |
Silon Taborex TA 2111 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1108 HD, TA 1109 HD. TA 2111 HD contains the cross-linking catalyst to complete together with the above-mentioned graft a S.. |
|||
Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | |
Silon Taborex TA 2120 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1104 HD, TA 1105 HD, TA 1116 HD. TA 2120 HD contains the cross-linking catalyst to complete together with the above-mention.. |
|||
Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | |
Silon Taborex TA 2121 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1105 HD, TA 1109 HD and TA 1117 HD. TA 2121 HD contains the cross-linking catalyst to complete together with the above-ment.. |
|||
Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | |
Silon Taborex TA 2126 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD, TA 1109 HD. TA 2126 HD contains the cross-linking catalyst to complete together with the above-mentioned graft a .. |
|||
Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | |
Silon Taborex TA 2143 HD Catalyst Masterbatch Masterbatch for the use with SILON PE-Xb Compounds TA 1108 HD, TA 1132 HD and TA 1134 HD. TABOREX TA 2143 HD contains a cross-linking catalyst and a part of the long term stabilising system for the .. |
|||
Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | ASTM D1895 |
Plenco 7080 Phenolic, Nodular, Compression Molded PLENCO 07080 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties along with outstanding resistance to cracking and degradation from soap and de.. |
|||
Bulk Density | 0.540 - 0.650 g/cc | 0.0195 - 0.0235 lb/in³ | |
Addcomp ADD-VANCE® Start & Stop Shutdown Masterbatch, PP base Fields of application: Stabilization master batch for polypropylene/polyethylene for stabilization of thermoplastic material in the extruder during shut-down periods to prevent formation of black sp.. |
|||
Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | |
Asahi Glass Fluon® CD1 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |
|||
Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | |
Asahi Glass Fluon® CD123 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |
|||
Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | |
Silon TA 2125 HD Natural Catalyst Masterbatch Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD. TA 2125 HD, together with the above mentioned graft, contains the cross-linking catalyst to complete a Sioplas System.. |