Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | Loose |
Nyco NYGLOS® 4W Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | Loose |
Nyco RRIMGLOS® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | |
Nabaltec APYRAL® 120E Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | |
Nabaltec APYRAL® 200 SM Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | |
Potters Industries Q-Cel® 5032S Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | |
NanoScale NanoActive® Aluminum Oxide Plus NanoActive Al2O3 Plus is produced using proprietary processes to obtain high specific surface area, high porosity (75% are mesopores), low density, weakly aggregated material possessing high adsorpt.. |
|||
Bulk Density | 0.200 - 0.450 g/cc | 0.00723 - 0.0163 lb/in³ | |
Magyar Aluminum ALOLT 90F Aluminum Hydroxide Fine Precipitated Type |
|||
Bulk Density | 0.200 - 0.500 g/cc | 0.00723 - 0.0181 lb/in³ | Loose |
Minelco UltraCarb LH15 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Bulk Density | 0.200 - 0.500 g/cc | 0.00723 - 0.0181 lb/in³ | Loose |
Minelco UltraCarb LH15C-10 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Bulk Density | 0.200 - 0.500 g/cc | 0.00723 - 0.0181 lb/in³ | Loose |
Minelco UltraCarb LH15X Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Bulk Density | 0.200 - 0.500 g/cc | 0.00723 - 0.0181 lb/in³ | Loose |
Minelco UltraCarb LH3 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Bulk Density | 0.200 - 0.400 g/cc | 0.00723 - 0.0145 lb/in³ | HG/T 2900 |
Shanghai Ofluorine T-2 PVDF for Powder Coatings Description: T-2 PVDF belong to thermoplastic fluorocarbon resin, which has high melt flow rate, low melt viscosity. T-2 PVDF has characteristic of chemical resistance, heat resistance, high mechani.. |
|||
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | |
Solvay GEROPON® SDS Surfactant Description: Sodium dioctylsulfosuccinate. Low rate, high performance, wetting agent for dry formulations.Identification: SODIUM DIOCTYLSULPHOSUCCINATECAS: 577 – 11 – 7Solubility: Soluble.. |
|||
Bulk Density | >= 0.200 g/cc | >= 0.00723 lb/in³ | Unpacked Bulk Density |
Zoltek Panex 35® Type 48 Chopped Carbon Fiber Chopped Carbon FiberApplications include: RFI/EMI shielding, mechanical wear resistance, weight reduction & dimensional stability |
|||
Bulk Density | 0.200 - 0.400 g/cc | 0.00723 - 0.0145 lb/in³ | |
Dow Corning EP-9289 LL Cosmetic Powder A white cross-linked dimethyl polysiloxane elastomer powder combined with lauroyl lysine. This unique combination enables the powder to improve flow and reduce agglomeration, providing superior hand.. |
|||
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | |
Chosun Refractories 1260PAPER Paper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | |
Chosun Refractories 1400BOARD Board Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | |
Chosun Refractories 1600HA BOARD Board Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | |
BASF Heligoen® Blue K 7090 Color Additive Chemical Structure: Cu-phthalocyanine betaApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PA, PETP, CA/CAB, and UPRecommendations for food applications: .. |
|||
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | Loose |
Nyco ULTRAFIBRE® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.200 g/cc | 0.00723 lb/in³ | |
BASF Paliotol™ Yellow K 1700 Color Additive Type of Pigment: Azo pigment, Ca/Na Lake Recommendations for food applications: Germany and FranceApplications: LDPE, HDPE/PP, PVC-P, PVC-U, PS, ABSInformation provided by BASF |