Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.330 - 0.390 g/cc | 0.0119 - 0.0141 lb/in³ | ASTM D1895 |
Polimeros Mexicanos Rotofoam® Plus 93050 Medium Density Polyethylene, Foam Grade Hexene Copolymer Linear Medium Density Polyethylene for foaming applications. It is formulated for inner layers with excellent foam cell structure and smooth surface finish and uniform closed cells... |
|||
Bulk Density | 0.330 - 0.390 g/cc | 0.0119 - 0.0141 lb/in³ | ASTM D1895 |
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized.Recommended for general purpose applications. Frequently used for water tanks (less tha.. |
|||
Bulk Density | 0.330 - 0.390 g/cc | 0.0119 - 0.0141 lb/in³ | ASTM D1895 |
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene MDPE Copolymer with UV8 stabilizer in natural and colors.Recommended for rotomolding. Used for manufacture of water tanks > 2000 liters, cisterns, farm tanks, or tanks to contain strong acids and b.. |
|||
Bulk Density | 0.330 - 0.390 g/cc | 0.0119 - 0.0141 lb/in³ | ASTM D1895 |
Polimeros Mexicanos Rotolene® Black Plus Polyethylene Polyethylene compound specially formulated for rotational molding applications requiring good mechanical properties and good mold release properties. Rotational molded parts have smooth surface and .. |
|||
Bulk Density | 0.330 - 0.390 g/cc | 0.0119 - 0.0141 lb/in³ | ASTM D1895-96 |
Polimeros Mexicanos Rotolene® Black Plus Ultra Polyethylene Linear copolymer Medium Density Polyethylene which is fully UV8 stabilized. Available as black powder.Applications: Polyethylene compound specially formulated for rotational molding applications req.. |
|||
Bulk Density | 0.330 - 0.390 g/cc | 0.0119 - 0.0141 lb/in³ | ASTM D1895 |
Polimeros Mexicanos Rotolene® Diesel Tank Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized.High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks a.. |
|||
Bulk Density | 0.290 - 0.390 g/cc | 0.0105 - 0.0141 lb/in³ | ASTM D1895 |
LG Chemical LK170 PVC General Description: LK170, vinyl chloride copolymer with vinyl acetate exhibit excellent properties including easy processing and effective flowMain Applications: Sealant, automotive protective sol.. |
|||
Bulk Density | 0.290 - 0.390 g/cc | 0.0105 - 0.0141 lb/in³ | ASTM D1895 |
LG Chemical LP090 PVC General Description: LP090 ,Homopolymer made from micro-suspension polymerization ,is a medium-viscosity PVC resin with a pseudo plastic flow property in processing range. LP090 can be used for wall.. |
|||
Bulk Density | 0.290 - 0.390 g/cc | 0.0105 - 0.0141 lb/in³ | ASTM D1895 |
LG Chemical LP170G PVC General Description: LP170G, homopolymer made from micro- suspension polymerization, is a low viscosity PVC resin with an good deaeration and stable viscosity at high temperature. Products made from.. |
|||
Bulk Density | 0.290 - 0.390 g/cc | 0.0105 - 0.0141 lb/in³ | ASTM D1895 |
LG Chemical LP170L PVC General Description: LP170L, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170L can be used for .. |
|||
Bulk Density | 0.0190 - 0.390 g/cc | 0.000686 - 0.0141 lb/in³ | Dependent on grade. |
Destech Open-Celled Glassy Carbon Foam Destech glassy (vitreous) carbon foam is available in different grades depending on the number of pores per inch (ppi). Standard grades are 10, 45, 100 and 500 ppi. Custom grades are available on a.. |