Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 3.97 g/cc | 0.143 lb/in³ | |
Astro Met AmAlOx 87 Alumina - Aluminum Oxide General Description:AmAlOx 87 alumina (Astro Met Aluminum Oxide) is a 99.95% alumina ceramic manufactured by Astro Met for specialty applications which require a higher purity of alumina than found .. |