Polymer Property : Bulk Density = 3.40 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 3.40 g/cc
0.123 lb/in³
Minelco MagnaDense 2 Fine Aggregate
MagnaDense is a high grade natural aggregate, manufactured from the iron oxide Magnetite. With its high density MagnaDense is used as loose ballast or as aggregate to produce high quality, high dens..
Bulk Density 3.40 g/cc
0.123 lb/in³
Minelco MagnaDense 4 Fine Aggregate
MagnaDense is a high grade natural aggregate, manufactured from the iron oxide Magnetite. With its high density MagnaDense is used as loose ballast or as aggregate to produce high quality, high dens..
Bulk Density 3.40 g/cc
0.123 lb/in³
China Tungsten YG13C Tungsten Carbide
Information provided by China Tungsten
Bulk Density 3.40 g/cc
0.123 lb/in³
China Tungsten YG4C Tungsten Carbide
Information provided by China Tungsten
Bulk Density 3.40 g/cc
0.123 lb/in³
China Tungsten YG6 Tungsten Carbide
Information provided by China Tungsten
Bulk Density 3.40 g/cc
0.123 lb/in³
Scott
China Tungsten YG6 Tungsten Carbide Powder
Information provided by China Tungsten
Bulk Density 3.40 g/cc
0.123 lb/in³
China Tungsten YG6C Tungsten Carbide
Information provided by China Tungsten
Bulk Density 3.40 g/cc
0.123 lb/in³
Scott
China Tungsten YG6C Tungsten Carbide Powder
Information provided by China Tungsten
Bulk Density 3.40 g/cc
0.123 lb/in³
China Tungsten YG8 Tungsten Carbide
Information provided by China Tungsten
Bulk Density 3.40 g/cc
0.123 lb/in³
China Tungsten YG8C Tungsten Carbide
Information provided by China Tungsten
Bulk Density 3.40 g/cc
0.123 lb/in³
Scott
China Tungsten YG6X Tungsten Carbide Powder
Information provided by China Tungsten