Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.76 g/cc | 0.0636 lb/in³ | |
Old Hickory M&M Clays, Inc. Wilco-SLU Kaolin Clay Wilco SLU is an aqueous suspension of kaolin produced at 70% solids content. The slurry is deflocculated and rheology stabilized with sodium silicate. The Wilco SLU grade is a highly permeable selec.. |
|||
Bulk Density | 1.76 - 1.81 g/cc | 0.0636 - 0.0654 lb/in³ | Precursor/core material (fine grained isotropic graphite) |
Destech Silicon Carbide, Solid or Foamed Destech silicon carbide foam is produced by chemical vapor reaction (CVR), in which high temperature silicon bearing gases convert glassy, or vitreous, carbon foam to SiC. Destech SiC foam has no c.. |