Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.675 g/cc | 0.0244 lb/in³ | ASTM D1895 |
Ascend Performance Materials Vydyne® 50BW NT0682 Nylon 66 Vydyne® 50BW NT0682 is a general-purpose, impact-modified PA66 resin. It is offered in natural and designed for extrusion-compounding applications. Vydyne 50BW NT0682 provides the chemical resistan.. |
|||
Bulk Density | 0.675 g/cc | 0.0244 lb/in³ | ASTM D1895 |
Ascend Performance Materials Vydyne® 50BW Nylon 66, General Purpose Vydyne® 50BW is a general-purpose PA66 resin. Offered in natural and designed for extrusion-compounding applications, this product is available at two moisture levels: 0.2% (max) as Vydyne 50BW and.. |