Polymer Property : Bulk Density = 0.640 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.640 g/cc
0.0231 lb/in³
Loose
Nyco 400 WOLLASTOCOAT® Wollastonite
This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make..
Bulk Density 0.640 g/cc
0.0231 lb/in³
Nabaltec APYRAL® 32 Al(OH)3
APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio..
Bulk Density 0.640 g/cc
0.0231 lb/in³
ASTM D1895
Plenco 2311 Phenolic, Granular, Injection Molded
PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr..
Bulk Density 0.640 g/cc
0.0231 lb/in³
ASTM D1895
Plenco 3509 Phenolic, Granular, Transfer Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..
Bulk Density 0.640 g/cc
0.0231 lb/in³
ASTM D1895
Plenco 3557 Phenolic, Granular, Compression Molded
PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r..
Bulk Density 0.640 g/cc
0.0231 lb/in³
ASTM D1895
Plenco 4349 Phenolic, Granular, Transfer Molded
PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer ..
Bulk Density 0.640 g/cc
0.0231 lb/in³
ASTM D1895
Plenco 4485 Phenolic, Granular, Injection Molded
PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a..
Bulk Density 0.640 g/cc
0.0231 lb/in³
ISO 60
Vyncolit X7012 Glass Fiber Reinforced Novolac Phenolic
Novolac resin based, glass fiber and glass beads reinforced. High mechanical strength even at high temperatures in Long Life CoolantsInformation provided by Sumitomo Bak North America, Inc.
Bulk Density 0.640 g/cc
0.0231 lb/in³
Zircar Ceramics IB-100B Alumina Bubble
Thin wall aluminum oxide ceramic spheres offered in 2 standard bubble sizes. These low density sintered ceramic bodies are useful in a range of refractory applications with temperatures to 2000°C (..
Bulk Density 0.640 g/cc
0.0231 lb/in³
ASTM D1895
Plenco 4309 Phenolic, Nodular, Injection Molded
PLENCO 04309 is a heat resistant, glass reinforced phenolic molding compound offering improved mechanical strength and electrical strength properties. UL recognized under component file E40654. 0430..
Bulk Density 0.640 g/cc
0.0231 lb/in³
pellets; ISO 60
Covestro Makrolon® 1952 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me..
Bulk Density 0.640 g/cc
0.0231 lb/in³
pellets; ISO 60
Covestro Makrolon® 2405 MAS056 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Bulk Density 0.640 g/cc
0.0231 lb/in³
pellets; ISO 60
Covestro Makrolon® 2405 MAS057 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Bulk Density 0.640 g/cc
0.0231 lb/in³
pellets; ISO 60
Covestro Makrolon® 2407 MAS056 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng..
Bulk Density 0.640 g/cc
0.0231 lb/in³
pellets; ISO 60
Covestro Makrolon® 2665 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy..
Bulk Density 0.640 g/cc
0.0231 lb/in³
pellets; ISO 60
Covestro Makrolon® 6255 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Lo..
Bulk Density 0.640 g/cc
0.0231 lb/in³
BASF Styropor® BF 422 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv..
Bulk Density 0.640 g/cc
0.0231 lb/in³
BASF Styropor® BFL 222 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c..
Bulk Density 0.640 g/cc
0.0231 lb/in³
BASF Styropor® BFL 322 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c..
Bulk Density 0.640 g/cc
0.0231 lb/in³
BASF Styropor® BFL 327 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c..
Bulk Density 0.640 g/cc
0.0231 lb/in³
BASF Styropor® BF 327 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv..
Bulk Density 0.640 - 0.740 g/cc
0.0231 - 0.0267 lb/in³
BASF Ultramid® B40 L PA6
Description: Ultramid® B40 L is a lubricated polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film and monofilaments. Product supplied in 2-2.5 mm round ..
Bulk Density 0.640 - 0.740 g/cc
0.0231 - 0.0267 lb/in³
BASF Ultramid® B40 PA6
Description: Ultramid® B40 is a polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film and monofilaments. Product supplied in 2-2.5 mm round pellets.Infor..
Bulk Density 0.640 g/cc
0.0231 lb/in³
BASF Styropor® BF 222 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv..
Bulk Density 0.640 - 0.740 g/cc
0.0231 - 0.0267 lb/in³
BASF Ultramid® B27 SD 02 PA6
Description: Ultramid® B27 SD 02 is a polyamide 6 for the production of semi dull textile and carpet fibers. Product comes in 2-2.5 mm cylindrical pellets.Information provided by BASF
Bulk Density 0.640 - 0.740 g/cc
0.0231 - 0.0267 lb/in³
BASF Ultramid® B33 L PA6
Description: Ultramid® B33 L is a lubricated polyamide 6 grade of intermediate viscosity that is well suited for the production of biaxial oriented and cast film and monofilaments. Product comes ..
Bulk Density 0.640 - 0.740 g/cc
0.0231 - 0.0267 lb/in³
BASF Ultramid® B33 LV PA6
Information provided by BASF
Bulk Density 0.640 g/cc
0.0231 lb/in³
BASF Styropor® BF 322 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv..
Bulk Density 0.640 - 0.740 g/cc
0.0231 - 0.0267 lb/in³
BASF Ultramid® B36 LN 01 PA6
Description: Ultramid® B36 LN 01 is a polyamide 6 grade of intermediate to high viscosity that is well suited for the production of cast and blown film. Clarity and thermoformability are enhanced b..