Physical Properties Metric English Comments
Bulk Density 0.375 g/cc
0.0135 lb/in³
Pour Density; ASTM D 1513
Orion Engineered Carbons DUREX® 0/35 Carbon Black
Specialty carbon black for technical rubber goods; Excellent extrusion propertiesProduced by Lamp Black processInformation provided by Orion Engineered Carbons.
Bulk Density 0.375 g/cc
0.0135 lb/in³
Pour Density; ASTM D 1513
Orion Engineered Carbons PUREX® HS 25 Carbon Black
Carbon black grade for manufacture of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons.
Bulk Density 0.375 - 0.575 g/cc
0.0135 - 0.0208 lb/in³
Shandong Dongyue Polymer DF-201 PTFE Fine Powder
Usage: It is suitable for making unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse..
Bulk Density 0.375 - 0.575 g/cc
0.0135 - 0.0208 lb/in³
Shandong Dongyue Polymer DF-202 PTFE Fine Powder
Usage: It is mainly used to process, belt, thin sheet and unsintered tape, thin wall rod etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF..
Bulk Density 0.375 - 0.575 g/cc
0.0135 - 0.0208 lb/in³
Shandong Dongyue Polymer DF-203 PTFE Fine Powder
Usage: The resin is used to process capillary tube, thin-wall tube, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside...
Bulk Density 0.375 - 0.575 g/cc
0.0135 - 0.0208 lb/in³
Shandong Dongyue Polymer DF-204 PTFE Fine Powder
Usage: The resin is mainly used for elastic tape, capillary tube, and the unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE s..
Bulk Density 0.375 g/cc
0.0135 lb/in³
Dry
Skamol Group V-1100 375 Vermiculite Insulating Slab
SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr..
Bulk Density 0.375 g/cc
0.0135 lb/in³
Dry
Skamol Group V-LITE 375 Vermiculite Insulating Brick
V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica..
Bulk Density 0.375 - 0.575 g/cc
0.0135 - 0.0208 lb/in³
Shandong Dongyue Polymer DF-205 PTFE Fine Powder
Usage: The resin is used to process two-side draw film, capillary tube, thin-wall tube, sheet, small-diameter rod, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC ba..
Bulk Density 0.375 g/cc
0.0135 lb/in³
ASTM D4894
3M Dyneon™ CC085 Custom Fluoropolymer Compound  (discontinued **)