Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.350 g/cc | 0.0126 lb/in³ | |
Nabaltec APYMAG® 80S Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Bulk Density | 0.350 g/cc | 0.0126 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® N 683 ASTM Carbon Black Standard grade of furnace black in accordance with the requirements of ASTM D 1765Soft Black - carcass grade, semi-reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | |
Pau Tai UNINOX PA-710 PVC Processing Aid UNINOX PA-710 is an acrylic lubricating process aid that offers significant berifits to processors of rigid PVC sheet, film, and molded products. This additive is designed to offer excellent clarity.. |
|||
Bulk Density | 0.350 - 0.500 g/cc | 0.0126 - 0.0181 lb/in³ | |
Magyar Aluminum Zeolite |
|||
Bulk Density | >= 0.350 g/cc | >= 0.0126 lb/in³ | LSY-QB-KD019 |
LG Chemical PA910 Processing aid Description: General purposeApplication: Sheet, window profile, pipe etcInformation provided by LG Chemical |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | |
Solvay Chemicals NOCOLOK® Flux Potassium Fluoroaluminate A high quality fluxing agent for brazing aluminum components. Classifications: HS No.: 38109090/CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration .. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | |
Solvay Chemicals NOCOLOK® Li Flux Flux for aluminum brazing with further reduced residue solubility and improved corrosion characteristics.HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air.. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | ASTM D-4894 |
Shamrock Technologies Fluoro T® 607 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | ASTM D-4894 |
Shamrock Technologies Fluoro T® 707 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | ASTM D-4894 |
Shamrock Technologies Fluoro T® 807 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | ASTM D-4894 |
Shamrock Technologies MicroFLON® 1437 Thermoplastic Grade PTFE Additive Used in high temperature engineering plastics.The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion... |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | |
Shandong Rike Chemical HELIâ„¢ HL-200 PVC Processing Aid Series (PA) Outline of ACR Processing AidsProducts of processing aid series developed by our company are acrylic copolymers. The basic function of processing aids is to improve processing performance and promo.. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | |
Shandong Rike Chemical HELIâ„¢ HL-230P PVC Processing Aid Series (PA) Outline of ACR Processing AidsProducts of processing aid series developed by our company are acrylic copolymers. The basic function of processing aids is to improve processing performance and promo.. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | |
Shandong Rike Chemical HELIâ„¢ HL-275P PVC Processing Aid Series (PA) Outline of ACR Processing AidsProducts of processing aid series developed by our company are acrylic copolymers. The basic function of processing aids is to improve processing performance and promo.. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | |
Shandong Rike Chemical HELIâ„¢ HL-530 PVC Foaming Regulator Outline of PVC Foaming Regulators:The HL-series PVC foaming regulators developed by our company are actually acrylic processing aids and have all characteristics of acrylic processing aids. The onl.. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | |
Shandong Rike Chemical HELIâ„¢ HL-755 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | |
Shandong Rike Chemical HELIâ„¢ HPA-41 PVC Processing Aid Series (PA) Outline of ACR Processing AidsProducts of processing aid series developed by our company are acrylic copolymers. The basic function of processing aids is to improve processing performance and promo.. |
|||
Bulk Density | 0.350 g/cc | 0.0126 lb/in³ | |
SGL Carbon Group SIGRAFIL C® C25 M100 UNS Milled Carbon Fiber, Unsized Carbon Fiber Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | ASTM D-4894 |
Shamrock Technologies Fluoro T® 602 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | ASTM D-4894 |
Shamrock Technologies Fluoro T® 603 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | |
Shandong Rike Chemical HELIâ„¢ HL-220N PVC Processing Aid Series (PA) Outline of ACR Processing AidsProducts of processing aid series developed by our company are acrylic copolymers. The basic function of processing aids is to improve processing performance and promo.. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | |
Shandong Rike Chemical HELIâ„¢ HL-531 PVC Foaming Regulator Outline of PVC Foaming Regulators:The HL-series PVC foaming regulators developed by our company are actually acrylic processing aids and have all characteristics of acrylic processing aids. The onl.. |
|||
Bulk Density | 0.350 - 0.450 g/cc | 0.0126 - 0.0163 lb/in³ | |
Trelleborg Fillite® 52/7S (355) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.350 - 0.450 g/cc | 0.0126 - 0.0163 lb/in³ | |
Trelleborg Fillite® FG (300) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.350 - 0.450 g/cc | 0.0126 - 0.0163 lb/in³ | |
Trelleborg Fillite® 106 Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.350 - 0.450 g/cc | 0.0126 - 0.0163 lb/in³ | |
Trelleborg Fillite® SG (500) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Bulk Density | 0.350 g/cc | 0.0126 lb/in³ | ASTM D894 |
Daikin POLYFLON M-111 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with extremely smooth and fine surface. Suited to making packing and gaskets since moldings have an especially go.. |
|||
Bulk Density | 0.350 g/cc | 0.0126 lb/in³ | |
BASF Theroplast® Blue 684 Color Additive Chemical Structure: AnthrachinonApplication: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by B.. |
|||
Bulk Density | 0.350 g/cc | 0.0126 lb/in³ | Tapped |
Nyco ULTRAFIBRE® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.350 - 0.550 g/cc | 0.0126 - 0.0199 lb/in³ | |
Shandong Rike Chemical HELI™ HL-225 PVC Processing Aid Series (PA) Outline of ACR Processing AidsProducts of processing aid series developed by our company are acrylic copolymers. The basic function of processing aids is to improve processing performance and promo.. |