Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 37.5 cm @Thickness 3.00 mm |
14.8 in @Thickness 0.118 in |
415°C nozzle, 200°C tool |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |