Polymer Property : Linear Mold Shrinkage, Transverse = 0.0044 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0044 cm/cm

@Time 86400 sec
0.0044 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp OFB32I PPS
LNP LUBRICOMP* OFB32I is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SA..
Linear Mold Shrinkage, Transverse 0.0044 cm/cm

@Time 86400 sec
0.0044 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP OX97635 PPS
LNP LUBRICOMP* OX97635 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0044 cm/cm

@Time 86400 sec
0.0044 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC
LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supp..
Linear Mold Shrinkage, Transverse 0.0044 cm/cm

@Time 86400 sec
0.0044 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific)
LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Transverse 0.0044 cm/cm

@Time 86400 sec
0.0044 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66
LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re..
Linear Mold Shrinkage, Transverse 0.0044 cm/cm

@Time 86400 sec
0.0044 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific)
LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Transverse 0.0044 cm/cm

@Time 86400 sec
0.0044 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC (Asia Pacific)
LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supp..
Linear Mold Shrinkage, Transverse 0.0044 cm/cm

@Time 86400 sec
0.0044 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66
LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Transverse 0.0044 cm/cm

@Time 86400 sec
0.0044 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Asia Pacific)
LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0044 cm/cm

@Time 86400 sec
0.0044 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC
LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated.