Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0036 - 0.0040 cm/cm @Time 86400 sec |
0.0036 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0036 - 0.0040 cm/cm @Time 86400 sec |
0.0036 - 0.0040 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0036 cm/cm @Time 86400 sec |
0.0036 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON EX99689C PEI LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |