Physical Properties Metric English Comments
Coating Weight >= 46.1 g/m²
>= 28.8 lb/ream
520
ExxonMobil Label-Lyte® 150 LL-302 White Opaque OPP Facestock
White, corona-treated polypropylene label facestock designed for rigid and semi-rigid pressure-sensitive applications requiring durability, opacity, and excellent graphic appeal. The treated, high ..
Coating Weight >= 46.1 g/m²
>= 28.8 lb/ream
520
ExxonMobil Label-Lyte® 50 LL-534 II Coated, Clear OPP Facestock
Coated, clear, polypropylene label facestock designed for demanding pressure-sensitive applications where good ink adhesion and high-speed performance are required. This film provides a "no label"..
Coating Weight >= 46.1 g/m²
>= 28.8 lb/ream
520
ExxonMobil Label-Lyte® 95 LP Coated, White Opaque OPP for Water-based Patch Label Applications
White, polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement on glass, metal, HDPE, and PET containers. It is designed to be used as a mon..
Coating Weight 46.1 g/m²
28.8 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 150LL-302 OPP Film
Product Description: A white, corona-treated polypropylene label facestock designed for rigid and semi-rigid pressure-sensitive applications requiring durability, opacity, and excellent graphic appe..
Coating Weight >= 46.1 g/m²
>= 28.8 lb/ream
520
ExxonMobil Label-Lyte® 65 LIM-301 White Opaque OPP Film for Injection Mold Label Applications
White, treated, polypropylene film designed for injection mold labeling. It provides the right combination of roughness, anti-static, printability, cutting, and stiffness properties for this demandi..
Copyright © lookpolymers.com All Rights Reserved