Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.00752 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 0.152 - 0.208 g/cc
0.00550 - 0.00752 lb/in³
Dry
Reade Advanced Materials Diatomaceous Earth (DE) (SiO2·nH2O)
Description: A naturally occurring mineral derived from microscopic in size fossilized remains of marine diatoms. It has high absorption, low bulk density and high brightness.A silica source in the ..
Density 0.128 - 0.208 g/cc
0.00463 - 0.00752 lb/in³
Monmouth Rubber & Plastics Durafoam™ DK4141 NEO/EPDM Polymeric Blend
Information provided by Monmouth Rubber & Plastics Corp.
Copyright © lookpolymers.com All Rights Reserved