Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.86 - 3.94 g/cc | 0.139 - 0.142 lb/in³ | Sintered |
Nabaltec GRANALOX® NM 9915 B Ceramic Body, Binder Free Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti.. |
|||
Density | 3.88 - 3.92 g/cc | 0.140 - 0.142 lb/in³ | Sintered |
Nabaltec GRANALOX® NM 9916 F Ceramic Body Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.90 - 3.92 g/cc | 0.141 - 0.142 lb/in³ | Sintered |
Nabaltec GRANALOX® NM 9922 B Ceramic Body, Binder Free Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti.. |
|||
Density | 3.86 - 3.92 g/cc | 0.139 - 0.142 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9922 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.88 - 3.92 g/cc | 0.140 - 0.142 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9922 I Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |