Polymer Property : Density = 0.0694 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.900 - 1.92 g/cc
0.0325 - 0.0694 lb/in³
Average value: 1.31 g/cc Grade Count:184
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Density 1.66 - 1.92 g/cc
0.0600 - 0.0694 lb/in³
Average value: 1.77 g/cc Grade Count:15
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum..
Density 1.88 - 1.92 g/cc
0.0679 - 0.0694 lb/in³
IEC 60811
Fainplast Compounds HAX HF 087/2 Halogen Free PVC
Filling and bedding
Density 1.88 - 1.92 g/cc
0.0679 - 0.0694 lb/in³
ISO 1183
Fainplast Compounds Hax™ HFC 0115/1 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding for tandem extrusion onlyInformation provided by Fainplast Compounds
Density 1.88 - 1.92 g/cc
0.0679 - 0.0694 lb/in³
ISO 1183
Fainplast Compounds Hax™ HFC 087/2 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding for tandem extrusion onlyInformation provided by Fainplast Compounds
Density 1.72 - 1.92 g/cc
0.0621 - 0.0694 lb/in³
Molded
Bulk Molding Compounds BMC T40(18)-LS Die Casting Replacement Grade Molding Compound
BMC T40(18)-LS is a low shrink compound designed as a direct replacement for aluminum die casting applications. T40(18)-LS is UL recognized. Excellent mechanical properties and dimensional stabili..
Density 1.72 - 1.92 g/cc
0.0621 - 0.0694 lb/in³
Molded
Bulk Molding Compounds BMC T40(18)V0 Die Casting Replacement Grade Molding Compound
BMC T40(18)V0 is a lower cost version of BMC T40(18) where a UL 5V rating is not necessary.
Density 1.79 - 1.92 g/cc
0.0647 - 0.0694 lb/in³
Molded
Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound
BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma..