Physical Properties Metric English Comments
Density 1.86 - 1.89 g/cc
0.0672 - 0.0683 lb/in³
Pyrotek Pyrocast AR Castable Refractory
Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro..
Density 1.86 - 1.89 g/cc
0.0672 - 0.0683 lb/in³
Pyrotek Pyrocast AR FINE Castable Refractory
Pyrocast AR Fine is a fine-grain fused silica castable, offering similar insulation properties, yet lighter weight that the Pyrocast AR formulation. Pyrocast AR Fine is suited for thin wall casting..
Density 1.86 - 1.89 g/cc
0.0672 - 0.0683 lb/in³
Pyrotek Pyrocast PCR Abrasion-Resistant Refractory Castable
Pyrocast PCR is an abrasion resistant, thermal shock resistant castable. It is suitable to give exceptional resistance for conditions such as rapid heating or rapid cooling.ApplicationsCarbon anode..
Density 1.45 - 1.89 g/cc
0.0524 - 0.0683 lb/in³
Average value: 1.74 g/cc Grade Count:14
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Density 1.52 - 1.89 g/cc
0.0549 - 0.0683 lb/in³
Average value: 1.69 g/cc Grade Count:24
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Density 1.69 - 1.89 g/cc
0.0611 - 0.0683 lb/in³
Molded
Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound
BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie..
Density 1.79 - 1.89 g/cc
0.0647 - 0.0683 lb/in³
Molded
Bulk Molding Compounds BMC T15(GPT) General Purpose Molding Compound
BMC T15(GPT) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPT) is well suited for injection, transfer or compression..
Density 1.69 - 1.89 g/cc
0.0611 - 0.0683 lb/in³
Molded
Bulk Molding Compounds BMC T45HT Automotive Grade Molding compound
BMC T45HT was designed for the very demanding applications of automotive under hood engine covers. It meets the GMP UP .007 specification for automotive under hood. BMC T45HT is a vinyl ester base..
Copyright © lookpolymers.com All Rights Reserved