Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.79 - 1.83 g/cc | 0.0647 - 0.0661 lb/in³ | ISO R 1183 |
Fainplast Compounds CRA 90 Flexible PVC, Flame Retardant Electrical Bedding Flame retardant bedding |
|||
Density | 1.49 - 1.83 g/cc | 0.0538 - 0.0661 lb/in³ | Average value: 1.64 g/cc Grade Count:36 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Density | 1.42 - 1.83 g/cc | 0.0514 - 0.0661 lb/in³ | Average value: 1.61 g/cc Grade Count:48 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |