Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.933 - 0.937 g/cc | 0.0337 - 0.0339 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4435S (35405) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.933 - 0.937 g/cc | 0.0337 - 0.0339 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4436S (35405) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.916 - 0.938 g/cc | 0.0331 - 0.0339 lb/in³ | Average value: 0.920 g/cc Grade Count:84 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |
|||
Density | 0.915 - 0.939 g/cc | 0.0331 - 0.0339 lb/in³ | Average value: 0.920 g/cc Grade Count:72 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Density | 0.929 - 0.938 g/cc | 0.0336 - 0.0339 lb/in³ | Average value: 0.934 g/cc Grade Count:21 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and.. |
|||
Density | 0.930 - 0.938 g/cc | 0.0336 - 0.0339 lb/in³ | RP-0549 |
Solvay RHODASURF® BC-420 Surfactant Chemical Name: TRIDECYL ALCOHOL ETHOXYLATEDCAS: 78330-21-9Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODASURF BC-420 is a low foaming wetting agents for texti.. |