Physical Properties Metric English Comments
Density 0.921 - 0.925 g/cc
0.0333 - 0.0334 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 4223T (23407) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.921 - 0.924 g/cc
0.0333 - 0.0334 lb/in³
ASTM D1505
Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding
The Trithene® SX 7010 resin is a medium molecular weight, low-density polyethylene (LDPE) which allows the production of flasks with an adequate combination of mechanical and impact strength, flexi..
Density 0.920 - 0.924 g/cc
0.0332 - 0.0334 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 4222M (224F7) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.921 - 0.925 g/cc
0.0333 - 0.0334 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 4223V (23416) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.922 - 0.925 g/cc
0.0333 - 0.0334 lb/in³
ASTM D1505
Petroquimica Triunfo Trithene® TS 7045 LDPE - Film - Plastification
The Trithene TS 7045 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..
Density 0.922 - 0.924 g/cc
0.0333 - 0.0334 lb/in³
ASTM D1505
Petroquimica Triunfo Trithene® TU 8091 LDPE - Agricultural Film
Trithene TU 8091 is a low-density polyethylene (LDPE) with high molecular weight, with excellent mechanical properties and good processability. These qualities ensure the production of very wide fil..
Density 0.922 - 0.924 g/cc
0.0333 - 0.0334 lb/in³
ASTM D1505
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film
The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This..
Density 0.9185 - 0.924 g/cc
0.03318 - 0.0334 lb/in³
Kazanorgsintez 102-05K Cable Composition Based on Low Density Polyethylene
Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca..
Density 0.918 - 0.924 g/cc
0.0332 - 0.0334 lb/in³
Kazanorgsintez 102-17 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Density 0.918 - 0.924 g/cc
0.0332 - 0.0334 lb/in³
Kazanorgsintez 102-23 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Density 0.918 - 0.924 g/cc
0.0332 - 0.0334 lb/in³
Kazanorgsintez 107-18 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Density 0.918 - 0.924 g/cc
0.0332 - 0.0334 lb/in³
Kazanorgsintez 107-19 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Density 0.918 - 0.924 g/cc
0.0332 - 0.0334 lb/in³
Kazanorgsintez 107-22 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Density 0.917 - 0.925 g/cc
0.0331 - 0.0334 lb/in³
Kazanorgsintez 107-276 Low Density Polyethylene Composition with Improved Processibility
Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez
Density 0.917 - 0.925 g/cc
0.0331 - 0.0334 lb/in³
Kazanorgsintez 107-277 Low Density Polyethylene Composition with Improved Processibility
Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez
Density 0.917 - 0.925 g/cc
0.0331 - 0.0334 lb/in³
Kazanorgsintez 107-278 Low Density Polyethylene Composition with Improved Processibility
Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez
Density 0.917 - 0.925 g/cc
0.0331 - 0.0334 lb/in³
Kazanorgsintez 108-276 Low Density Polyethylene Composition with Improved Processibility
Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez
Density 0.917 - 0.925 g/cc
0.0331 - 0.0334 lb/in³
Kazanorgsintez 108-277 Low Density Polyethylene Composition with Improved Processibility
Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez
Density 0.9185 - 0.924 g/cc
0.03318 - 0.0334 lb/in³
Kazanorgsintez 153-03K Cable Composition Based on Low Density Polyethylene
Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca..
Density 0.9185 - 0.924 g/cc
0.03318 - 0.0334 lb/in³
Kazanorgsintez 153-05K Cable Composition Based on Low Density Polyethylene
Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca..
Density 0.917 - 0.925 g/cc
0.0331 - 0.0334 lb/in³
Kazanorgsintez 158-280 Low Density Polyethylene Composition with Improved Processibility
Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez
Density 0.917 - 0.925 g/cc
0.0331 - 0.0334 lb/in³
Kazanorgsintez 158-281 Low Density Polyethylene Composition with Improved Processibility
Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez
Density 0.917 - 0.925 g/cc
0.0331 - 0.0334 lb/in³
Kazanorgsintez 162-280 Low Density Polyethylene Composition with Improved Processibility
Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez
Density 0.917 - 0.925 g/cc
0.0331 - 0.0334 lb/in³
Kazanorgsintez 162-281 Low Density Polyethylene Composition with Improved Processibility
Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez
Density 0.917 - 0.925 g/cc
0.0331 - 0.0334 lb/in³
Kazanorgsintez 108-278 Low Density Polyethylene Composition with Improved Processibility
Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez
Density 0.917 - 0.925 g/cc
0.0331 - 0.0334 lb/in³
Kazanorgsintez 108-279 Low Density Polyethylene Composition with Improved Processibility
Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez
Density 0.919 - 0.925 g/cc
0.0332 - 0.0334 lb/in³
BRCP 4843
ExxonMobil Jayflex™ DINA Plasticizer
Appearance: Clear and FreeAvailability: North AmericaCAS Number: 33703-08-01Information provided by ExxonMobil
Density 0.916 - 0.925 g/cc
0.0331 - 0.0334 lb/in³
Average value: 0.920 g/cc Grade Count:34
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum..
Density 0.922 - 0.925 g/cc
0.0333 - 0.0334 lb/in³
ASTM D1505
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification
The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..
Density 0.918 - 0.924 g/cc
0.0332 - 0.0334 lb/in³
Kazanorgsintez 153-16 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Copyright © lookpolymers.com All Rights Reserved