Physical Properties Metric English Comments
Density 0.857 - 0.913 g/cc
0.0310 - 0.0330 lb/in³
ASTM D792
Dow Engage® Polyolefin Elastomer
Engage® thermoplastic elastomers are ethylene octene copolymers produced via advanced INSITE™ catalyst and process technology, allowing control over polymer structure, properties, and rheology. ..
Density 0.849 - 0.913 g/cc
0.0307 - 0.0330 lb/in³
CMT Materials HYTAC® WF High Strength High Clarity 450°F Epoxy Syntactic
HYTAC-WF is an excellent high temperature epoxy syntactic material that provides improved clarity when forming APET and other clear polymers plus reduces sticking of difficult to process polymers su..
Density 0.833 - 0.913 g/cc
0.0301 - 0.0330 lb/in³
Average value: 0.847 g/cc Grade Count:12
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..