Physical Properties Metric English Comments
Density 0.570 - 0.630 g/cc
0.0206 - 0.0228 lb/in³
True, 3M QCM 14.24.6
3M HGS10000 Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..
Density 0.570 - 0.630 g/cc
0.0206 - 0.0228 lb/in³
True, 3M QCM 14.24.6
3M HGS18000 Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..
Density 0.570 - 0.630 g/cc
0.0206 - 0.0228 lb/in³
3M iM30K Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.570 - 0.630 g/cc
0.0206 - 0.0228 lb/in³
3M S60HS Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.570 - 0.630 g/cc
0.0206 - 0.0228 lb/in³
3M S60 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..