Polymer Property : Density = 0.00253 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0500 - 0.0700 g/cc
0.00181 - 0.00253 lb/in³
ISO 845-88
Eurofoam Porocell POR 300/60 Ethylene Octane Metallocene EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Density 0.0600 - 0.0700 g/cc
0.00217 - 0.00253 lb/in³
typical range; ISO 845
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..