Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 18.0 g/cc | 0.650 lb/in³ | |
Hogen HM3000 Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a l.. |
|||
Density | 18.0 g/cc | 0.650 lb/in³ | |
Hogen HM3050 Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE.. |
|||
Density | 18.0 g/cc | 0.650 lb/in³ | |
Mi-Tech Metals HD18 Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high therm.. |
|||
Density | 18.0 g/cc | 0.650 lb/in³ | |
Mi-Tech Metals HD18D Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con.. |
|||
Density | 18.0 g/cc | 0.650 lb/in³ | |
Wieland Porta P6 PFM Alloy Gold-platinum-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneeringDental |
|||
Density | 18.0 g/cc | 0.650 lb/in³ | |
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Density | 18.0 g/cc | 0.650 lb/in³ | |
CMW® 3950 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |